Firing float glass

Postby BobbieMatus » Sun Oct 12, 2003 7:21 pm

I need to fire a 16" round circle made of float glass. What temperture do I need to go to and what temperture to anneal at??? Also how long for the annealing. Thanks for your help have been working only with spectrum and some bullseye.

Barbara Cashman
Posts: 151
Joined: Sun Mar 09, 2003 5:42 pm
Location: Greensboro NC
Contact:

Postby Barbara Cashman » Sun Oct 12, 2003 7:26 pm

You didn't say if there was more than one layer, and the thickness of it or each. also, are you fusing or slumping. Need a little more info. - Barbara

BobbieMatus
Posts: 50
Joined: Tue Jul 08, 2003 12:21 am

Postby BobbieMatus » Mon Oct 13, 2003 10:03 am

I am using two pieces of double strength float glass. Would like to fuse it and then slump it in a separate firing.
Bobbie

Bert Weiss
Posts: 2338
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Postby Bert Weiss » Mon Oct 13, 2003 5:38 pm

luvhug wrote:I am using two pieces of double strength float glass. Would like to fuse it and then slump it in a separate firing.
Bobbie


Use Borax on top. Fire to 1240 and soak for an hour then to 1420 with a 20 minute hold and shut off. It should anneal. I'd try tin sides in the center with that schedule.

Make the texture underneath it interesting.

For the slump, It sort of depends on the mold etc. I have no experience working with double strength. I'd probably fire it to 1300 for 10 minutes, but that is an outside guess. You have to look and see what's doing.

The heating rate is totally dependent on your kiln setup. I go up at 600º per hour. You might not be able to.

Bert
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 39 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com