Post by Val »

Can anybody tell me if I can use 90 coe confetti with 96 in a tack fuse, also is 96 confetti available? I would like to know before I go out and buy some.

Val
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: Confetti

Post by Brock »

Val wrote:Can anybody tell me if I can use 90 coe confetti with 96 in a tack fuse, also is 96 confetti available? I would like to know before I go out and buy some.

Val
Possibly. The worst that will happen, is that the confetti may flake off the substrate. There will not be enough voliume of confetti to break the piece.
My memory is so good, I can't remember the last time I forgot something . . .
Val
Posts: 35
Joined: Sun May 25, 2003 8:01 pm
Contact:

Post by Val »

Thanks Brock,
I think I will buy a small amount and experiment.

Val
LDGlass
Posts: 22
Joined: Sun Mar 23, 2003 2:54 pm
Location: Milwaukee, WI
Contact:

Post by LDGlass »

I took a look at your website Val... I love those little people that hold notes and photographs! How clever!!! :D


Laura
http://www.glasscatjewels.com
Val
Posts: 35
Joined: Sun May 25, 2003 8:01 pm
Contact:

Post by Val »

Glad you like my "HIGgies", Laura, I haven't had time to update my site recently but look back in the future and see what I've been busy creating.