smcintyre

Lables on Bottles

Postby smcintyre » Mon Oct 27, 2003 1:22 pm

I see where people have labels on the bottles they slump. Can someone please tell me how this is accomplished? One person mentioned decals? Any suggestions will be greatly appreciated! Thanks, Suzette

Brad Walker
Site Admin
Posts: 1363
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Labels on Bottles

Postby Brad Walker » Mon Oct 27, 2003 1:46 pm

smcintyre wrote:I see where people have labels on the bottles they slump. Can someone please tell me how this is accomplished? One person mentioned decals? Any suggestions will be greatly appreciated! Thanks, Suzette


The labels are applied after the bottle has been slumped. They're sometimes soaked off before slumping and saved; sometimes a special label is created. Usually they're just glued on.

smcintyre

Postby smcintyre » Mon Oct 27, 2003 2:39 pm

Thank you so much. Someone mentioned something about ceramic decals. Do you know about these and where I can get the paper?

Thanks, Suzette

charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Postby charlie » Mon Oct 27, 2003 3:02 pm

anyone got a good tip for removing the labels in the first place? i've tried soaking, razor blades, chemicals, etc and nothing works well. what happens when you don't take it off? does it burn up completely without leaving traces? :?:

Judy Schnabel
Posts: 195
Joined: Mon Mar 10, 2003 9:45 pm
Location: SW FL
Contact:

labels on bottles

Postby Judy Schnabel » Mon Oct 27, 2003 3:32 pm

Charlie,

Never tried "burning" one off.

Most labels will come off after they've been soaked in water overnight. Some come off a lot easier than others.

Jack Daniels & Jose Guervo are tough. You have to keep "slicing" under the label with a scraper. Bacardi can be "peeled" off but you have to immediately put it on plain white paper to keep it safe. Stoli practically floats.

It's not a good idea to put the bottles (with labels on them) in hot water. That can discolor the label.

Hope this helps.

Judy

Judy Schnabel
Posts: 195
Joined: Mon Mar 10, 2003 9:45 pm
Location: SW FL
Contact:

labels on bottles

Postby Judy Schnabel » Mon Oct 27, 2003 3:35 pm

Charlie,

Never tried "burning" one off.

Most labels will come off after they've been soaked in water overnight. Some come off a lot easier than others.

Jack Daniels & Jose Guervo are tough. You have to keep "slicing" under the label with a scraper. Bacardi can be "peeled" off but you have to immediately put it on plain white paper to keep it safe. Stoli practically floats off.

It's not a good idea to put the bottles (with labels on them) in hot water. That can discolor the label.

Also, keep the bucket you're soaking them in out of the sun. The sun can discolor the label also.

Hope this helps.

Judy

charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: labels on bottles

Postby charlie » Mon Oct 27, 2003 3:55 pm

Judy Schnabel wrote:Charlie,

Never tried "burning" one off.

Most labels will come off after they've been soaked in water overnight. Some come off a lot easier than others.

Jack Daniels & Jose Guervo are tough. You have to keep "slicing" under the label with a scraper. Bacardi can be "peeled" off but you have to immediately put it on plain white paper to keep it safe. Stoli practically floats off.

It's not a good idea to put the bottles (with labels on them) in hot water. That can discolor the label.

Also, keep the bucket you're soaking them in out of the sun. The sun can discolor the label also.

Hope this helps.

Judy


thanks.

i'm not trying to save the labels. i've soaked wine bottles for a week with almost no affect. the adhesive seems to be not water based, so isn't really affected. the paper sort of dissolves over time, but it leaves the backing that i have to razor off or dissolve, which is a large bother. i was hoping for a magic incantation besides elbow grease.

Brad Walker
Site Admin
Posts: 1363
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: labels on bottles

Postby Brad Walker » Mon Oct 27, 2003 4:11 pm

charlie wrote:i was hoping for a magic incantation besides elbow grease.


Well, it's not magic, but try heating the labels with a hairdryer. Most of the glues are sensitive to heat and will come loose.

Rebecca M.
Posts: 126
Joined: Fri Sep 12, 2003 12:15 pm
Location: Myrtle Beach
Contact:

Postby Rebecca M. » Mon Oct 27, 2003 4:26 pm

I did one that was a beezer to get the label and glue off. I used a razor blade for most of it and Goo-Gone with a scrubbie got the rest of the glue. It wasn't a paper label, but some sort of plastic.

Judy Schnabel
Posts: 195
Joined: Mon Mar 10, 2003 9:45 pm
Location: SW FL
Contact:

Labels

Postby Judy Schnabel » Mon Oct 27, 2003 4:30 pm

To get the final residue off, use oven cleaner. Spray on and leave for a few hours. Then go over that with Comet Cleanser. Try to purchase the oven cleaner that doesn't smell.

Judy

Judd
Posts: 291
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Postby Judd » Mon Oct 27, 2003 5:35 pm

Judy Schnabel,

This process works with Skyy Blue Vodka? Their little bottle, the six pack of Skyy Blue, are a BUGGER to remove labels from. I've tried lighter fluid, and it does not even begin to remove all the goo.

Charlie,

I've fired a few small (very small) pieces with a little goo on them still. I didn't notice a big difference between the totally cleaned and slightly gooey pieces. But, maybe I just got lucky.

Judd

Mark Kemp
Posts: 59
Joined: Mon Mar 10, 2003 11:57 am
Location: Corvallis, Oregon
Contact:

Postby Mark Kemp » Mon Oct 27, 2003 7:22 pm

Orange oil, such as Citrisolv, works well on a lot of label adhesive. Softens it, then it can be removed with a strong detergent solution.

Judy Schnabel
Posts: 195
Joined: Mon Mar 10, 2003 9:45 pm
Location: SW FL
Contact:

labels

Postby Judy Schnabel » Mon Oct 27, 2003 7:57 pm

Skyy vodka bottles are a challenge. After I pull the silver top portion off I spray oven cleaner on what's left of the label. I usually leave them sit overnight. Then I start with the scraper and Comet Cleanser. That usually works for me.

I've also been introduced to a product called "un-du" which can be purchased at Wal-Mart in the area for scrappers (people who do scrap books). I've used it on Yellow Tail (I believe) and got the label off in one piece.

Judy

Carol
Posts: 112
Joined: Sun Mar 09, 2003 5:48 pm
Location: Thetis Island, BC, Canada
Contact:

Postby Carol » Mon Oct 27, 2003 8:28 pm

charlie wrote:anyone got a good tip for removing the labels in the first place? i've tried soaking, razor blades, chemicals, etc and nothing works well. what happens when you don't take it off? does it burn up completely without leaving traces? :?:


Experience will show you which labels soak off easily. I've generally found that most imported wines have water soluble glue. Fill up the sink at night, they've soaked off by am. I don't save the labels either and have narrowed my slumping to a couple of brands which require little or no elbow grease.

C.

BobbieMatus
Posts: 50
Joined: Tue Jul 08, 2003 12:21 am

Postby BobbieMatus » Mon Oct 27, 2003 9:36 pm

Soaking and razor blades is what I use. Don't try to burn off in kiln, any glue that wasn't cleaned off will leave traces on finished bottle
Bobbie

J. Savina
Posts: 18
Joined: Thu Mar 27, 2003 2:28 pm
Location: DeMotte, Indiana
Contact:

Postby J. Savina » Mon Oct 27, 2003 11:24 pm

charlie wrote:anyone got a good tip for removing the labels in the first place? i've tried soaking, razor blades, chemicals, etc and nothing works well. what happens when you don't take it off? does it burn up completely without leaving traces? :?:


What kind of chemicals are you using. I just use Goo Gone or Goof Off. Soak for a bit and the label comes right off. I get it at Home Depot.
Jeanette S. Cobb
J. Savina Stained Glass Studio

quill
Posts: 107
Joined: Wed Apr 02, 2003 10:35 am
Location: BC
Contact:

Postby quill » Tue Oct 28, 2003 12:30 am

I see where people have labels on the bottles they slump. Can someone please tell me how this is accomplished? One person mentioned decals? Any suggestions will be greatly appreciated! Thanks, Suzette


HI Suzette,
I have had no luck with saving labels, (I have not slumped bottles but used to remove them when I was doing glass repairs.

What does work for me is searching ebay for labels. You can buy vintage & current bottle labels there from various sellers.
Good luck & hope this helps.

Gale aka artistefem
Posts: 184
Joined: Sun Mar 09, 2003 8:14 pm
Location: MO-on the banks of the Mississippi
Contact:

Postby Gale aka artistefem » Tue Oct 28, 2003 8:50 am

I do a razor blade or fingernail test on the edge of the label to check what kind of adhsive has been used to affix the label.

All the water soaking in the world won't take off the gum adhesives. To get this type of label off, I set my heat gun on low and carefully - moving quickly - warm the label, peeling as I heat. This works well. But if you use a heat gun - be careful not to apply so much heat that you thermal shock the bottle into shards.

A thorough clean-up is necessary of the label glue residue and the bottle neck where the neck label or metal capping has been applied. I use a solvent (with mild scratchy action) followed by a dishsoap bath and clear water rinse. Most likely if you try to burn a label off in the kiln, you will end up with devit.

Some of the bottles my friends give me are heavily streaked on the outside with wine trails and need extra cleaning, especially around the neck area. These must be the last "flight" of bottles opened during their wine toasting parties - LOL!


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 31 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com