I can't find the reason for my devit problem

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
lucho/lachezar/
Posts: 15
Joined: Tue Aug 03, 2004 12:46 pm
Location: bulgaria
Contact:

Re: I can't find the reason for my devit problem

Post by lucho/lachezar/ »

Can you say if your kiln is responding accordingly to the program? If only one element is gone or one phase (in 3 phase circuits) is low (voltage) or bad contact it may cause temperature differences in the kiln beyond the thermo-couple ability to read...

Then following Cynthia's, post I used to have problems with glass wrapped in paper and in wooden boxes and exposed to rain...

Lucho