Can you leave waxed paper in kiln?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Faye Malench
Posts: 46
Joined: Sun Jan 02, 2005 9:03 pm
Location: Illinois
Contact:

Re: Can you leave waxed paper in kiln?

Post by Faye Malench »

I thought about waxed paper since I recall people gluing snowflake bits to them. I assumed they were then fired. Also, have butcher's paper - waxed on one side. No, I don't want the spray to creep under for sure and the waxed paper would cause that. I can protect the elements with a sleeve of cardboard around the piece so spray doesn't drift.
Post Reply