Postby daffodildeb » Fri Nov 28, 2003 7:35 pm

I've seen some beautiful dichroic glass pendants, and I'm trying to figure out how they are made. They are obviously layered, somewhat at random, and then cut into shapes with a channel for a chain or cord.

I know how to make the channel, but I haven't been able to figure out how to make nice shapes other than squares and triangles. How do you make pretty curves, etc., with layers of dichro. I believe they might be made of larger panels of dichro and other glass.

This may be a stupid question but I'd really like to know! :oops:
Deb

Dolores
Posts: 106
Joined: Mon Jul 14, 2003 9:21 pm
Location: Sunny Southern California
Contact:

Postby Dolores » Sat Nov 29, 2003 12:50 am

Deb,

coldwork, coldwork, coldwork! I couldn't live without my Inland disc grinder and glass grinder. I also make good use of my Taurus II ringsaw. After all the manipulating, a nice gentle fire polish brings back the shine. With the proper equipment, there really is no limit as to the shapes or designs one can conjure up! Let's not forget wet belt sanders, lap machines, dremel tools, and tile saws. Also sandblasting units, tumblers, vibratory laps, acid etching, oil polish, spit... etc...etc...
BOTTOM LINE: Fusing the glass is only the beginning of the work!

DOLORES

Kitty
Posts: 437
Joined: Sun Mar 09, 2003 4:12 pm
Location: Gig Harbor, WA

Postby Kitty » Sat Nov 29, 2003 5:59 am

casting the channel and also having intricate curves in the same pendant is a tall order. basic shapes - squares, rectangles - are easily done with the channel.

but if drilling holes, i guess any shape could be cut out, fire polished, and hung on a necklace.

Peg
Posts: 74
Joined: Tue Apr 08, 2003 7:50 am
Location: Bristol, UK

Postby Peg » Wed Dec 03, 2003 8:03 am

Fire hot enough and you'll get rounded corners if the item is thick enough. Small (15mm) square, 6mm thick will become a circle. (Hotish = 836 C).
This isn't infallible, but half the fun is not knowing what you'll find when you open the kiln door...

Robert Cohen

Pendant shapes

Postby Robert Cohen » Wed Dec 03, 2003 9:35 am

Fuse three layers of glass -- base, dichroic middle layer and clear cap. Lay out a design on the fused piece using either a template or your imagination and then grind to shape. Fire polish your product and you have your dichroic pendant.

molly
Posts: 69
Joined: Tue Jul 15, 2003 7:38 pm

Postby molly » Wed Dec 03, 2003 2:16 pm

Is the channel just made with a steady hand and diamond point bit? I am unsure just how channeling is done. Anybody wanna help me?

charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Postby charlie » Wed Dec 03, 2003 2:23 pm

channel bit on a grinder

Kitty
Posts: 437
Joined: Sun Mar 09, 2003 4:12 pm
Location: Gig Harbor, WA

Postby Kitty » Wed Dec 03, 2003 2:25 pm

molly, there is quite a bit in the archives about how to cast a channel in a pendant, so a cord can slide thru. people do it with fiber paper, or with a thin welding rod coated in kiln wash or bead release. see if you can find some of those previous posts ... it's been described in pretty good detail a number of time. good luck. come back if you can't round up the info.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: Google [Bot], Majestic-12 [Bot] and 66 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com