Postby Cheryl » Mon Dec 08, 2003 4:58 pm

Was online looking for rectangular shelves to chop up when I stumbled on these. They're pretty pricey, but otherwise sound terrific!

http://www.baileypottery.com/kilnfurnit ... helves.htm

Barbara Muth
Posts: 382
Joined: Sun Mar 09, 2003 8:10 pm
Location: Washington DC Metropolitan Area
Contact:

Postby Barbara Muth » Mon Dec 08, 2003 5:09 pm

yah but if it has absorbed any moisture it explodes unless you ramp up verrrry slowly.

that's a shame.

Barbara
Barbara
Check out the glass manufacturer's recommended firing schedules...
LATEST GLASS

Terry Ow-Wing
Posts: 124
Joined: Sun Mar 09, 2003 3:21 pm
Location: San Francisco, Ca.
Contact:

Postby Terry Ow-Wing » Mon Dec 08, 2003 10:07 pm

I actually have some samples of them. The company that sent it to me was not familiar with any glass users. So far my 2 test of point loads of 4 layers of glass on one spot has had them survive. I just have not had anytime to really go at it though. Interesting about exploding - where did you find this out?

[/quote]
Terry Ow-Wing Designs
Kilnformed and Lampworked Glass Art
http://GlassArt.weebly.com
Image

Susan Moore
Posts: 96
Joined: Mon Oct 06, 2003 10:07 pm
Location: Austin, TX
Contact:

Postby Susan Moore » Mon Dec 08, 2003 11:41 pm

If you scroll down to the bottom of their website there is a warning about the moisture/exploding issue.

Susan

Nikki ONeill
Posts: 165
Joined: Mon Mar 10, 2003 11:55 am
Location: Silver Spring, MD
Contact:

Postby Nikki ONeill » Tue Dec 09, 2003 11:26 am

I talked to a rep at Bailey who told me that the Advantage shelves are meant to be used only above 1800 degrees, in a reducing atmosphere. They will deteriorate if used at lower tempertures. Evidently the components in the shelf must re-form and that only happens at the higher temperatures. However there is an even more expensive material that can be special ordered that is oxidation resistant. I'll post more info if it looks good.
Nikki

Cheryl
Posts: 239
Joined: Sun Mar 09, 2003 7:56 pm
Location: Tallahassee FL
Contact:

explosion warnings

Postby Cheryl » Tue Dec 09, 2003 1:23 pm

posted right on the web site. Of course, we have similar problems with trapped water so I wasn't horribly put off by it. Then again, I NEVER "know better."


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 44 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com