Postby pclark » Tue Jan 13, 2004 2:33 am

Anyone know where to obtain optically clear glass? I am looking for something 1/4 inch to 1/2 inch in thickness. Almost like float but no tent. I know PPG makes Starphire but, have found no good source. Not sure if anyone else makes it or not. I see it all the time as dividers in resteraunts. Any help would be appreciated. Thanks.....

ellen abbott
Posts: 148
Joined: Tue Mar 11, 2003 12:04 pm
Location: Houston Tx
Contact:

Postby ellen abbott » Tue Jan 13, 2004 11:10 am

Glass Wholesalers in Houston carries it.

E

charlie holden
Posts: 260
Joined: Thu Mar 13, 2003 8:26 pm
Location: Atlanta

Postby charlie holden » Tue Jan 13, 2004 11:10 am

What you're seeing in restaurants is probably Starphire. If you call PPG they will tell you who their local distributors are.

It is also possible that what your seeing in restaurants is normal old float with moody lighting. You can minimize the green cast with a colored light. Flourescents make it worse.

ch

Glenda Kronke
Posts: 64
Joined: Tue Mar 11, 2003 11:44 am
Location: Austin, TX
Contact:

Clear glass

Postby Glenda Kronke » Wed Jan 14, 2004 2:20 pm

FYI- was just reading in Dec. issue of Glass Magazine about 'low-iron glass' by Guardian Industries Corp. "...introducing UltraWhite low-iron glass, a clear, high visible-light transmission glass.... UltraWhite's colorless appearance makes it applicable in a variety of commercial and residential applications....."

http://www.guardian.com

Might be worth asking for a sample.

Another 'clear' glass goes by the name of 'Diamante'. Call your local wholesaler and see if they carry it.

Hope this helps.

scooter riegelsperger
Posts: 26
Joined: Fri Mar 14, 2003 9:23 am
Location: Houston,TX
Contact:

Postby scooter riegelsperger » Wed Jan 14, 2004 2:59 pm

Another option in low-iron float is a product called optiwhite. I buy from Howard Glass in Worcester, MA. 508-753-8146 Talk to Jason. I think it's a little better than Starphire for clarity. It's available in 2,3,4,5,6,8,&10mm thick.
Do illiterate people get the full effect of alphabet soup?

Ron Coleman
Posts: 468
Joined: Sun Mar 09, 2003 3:20 pm
Location: Columbus, Ohio USA

Postby Ron Coleman » Wed Jan 14, 2004 5:16 pm


charlie holden
Posts: 260
Joined: Thu Mar 13, 2003 8:26 pm
Location: Atlanta

Postby charlie holden » Wed Jan 14, 2004 5:42 pm


pclark
Posts: 34
Joined: Fri Mar 14, 2003 7:31 pm
Location: Fort Worth Texas

Thanks...

Postby pclark » Thu Jan 15, 2004 1:23 am

Thanks for all the input. I will check on these leads! Happy Glassing.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 34 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com