Sean Albert
Posts: 8
Joined: Wed Dec 10, 2003 7:04 pm
Location: Alfred, NY

Schedule: is it to slow?

Post by Sean Albert »

I wrote in a few weeks ago about having trouble with BE devitrifying in an older kiln. I brought the kiln up to a high temp to “cleanâ€
Catharine Newell
Posts: 83
Joined: Thu Mar 13, 2003 12:33 am
Location: Portland, OR

Re: Schedule: is it to slow?

Post by Catharine Newell »

[quote="Sean Albert"]I wrote in a few weeks ago about having trouble with BE devitrifying in an older kiln. I brought the kiln up to a high temp to “cleanâ€
Catharine Newell
Posts: 83
Joined: Thu Mar 13, 2003 12:33 am
Location: Portland, OR

Post by Catharine Newell »

And.... ramp up AFAP from 1240 (or whatever works for you) to your full fuse - again, taking the work quickly thru the 1300 devit range. Don't dilly dally there!

Catharine
Sean Albert
Posts: 8
Joined: Wed Dec 10, 2003 7:04 pm
Location: Alfred, NY

Post by Sean Albert »

Thanks so much Catharine, I'll give it a try and let you know how it turns out. Sean.