new moldmaking material

Postby Patti S » Mon Mar 10, 2003 9:58 pm

http://www.glasscolor.com/catalog/casti ... otInst.asp

OCR has it on sale right now. The product sheet says it can be used for multiple firings, especially if kilnwashed. Has anyone tried this stuff yet?

Colin & Helen

Postby Colin & Helen » Tue Mar 11, 2003 12:20 am

No not as yet.. it sounds like the best thin since sliced bread.. I bet it won't be sold in my neck of the woods..Colin

Carolyn Ledbetter
Posts: 17
Joined: Mon Mar 10, 2003 1:29 pm
Location: Venice, Florida

Postby Carolyn Ledbetter » Tue Mar 11, 2003 11:55 am

Sounds interesting! Hope someone tries it out and posts their results. I've not had much sucess with damp mold materials. They were hard to work with and very stinky!

Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Postby Brock » Tue Mar 11, 2003 12:14 pm

It sounds like a new, and even more expensive, variation of HydraPerm, available through U.S. Gypsum.

Brock


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 11 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com