Post by slats »

Where can I find a supplier for powders for float glass. C&R Loo has just about exhausted their supply?
Tyler Frisby
Posts: 75
Joined: Tue Dec 02, 2003 8:27 pm
Location: Canada

Post by Tyler Frisby »

I dont know where to get it But I have Hotline Powders, for all I know its the same stuff.

Hope I helped

Tyler
PaulS
Posts: 155
Joined: Mon Mar 10, 2003 6:45 pm
Location: Belize
Contact:

Post by PaulS »

You have a supplier of Bohle products in the US, cos I've seen it mentioned before.

On their website you can see Frit clear COE 82;
http://www.bohle.de/scripts/mgrqispi.dl ... TS=-N2,-N2
and Confetti COE 82;
http://www.bohle.de/scripts/mgrqispi.dl ... TS=-N2,-N2
It ain't where you're from, it's where you're at!
mikefromitaly
Posts: 67
Joined: Thu Apr 03, 2003 7:47 am
Location: italy-sicily
Contact:

from Jim

Post by mikefromitaly »

you can find hotline from jim shaffer from ed hoys intl or by his dealers
mike from italy.
Gordon Exon
Posts: 5
Joined: Mon Feb 02, 2004 8:22 pm
Location: Calgary

Float Glass powders

Post by Gordon Exon »

Try Ferro their 80 683 water base or 270 oil base