Postby Marilyn Kaminski » Tue Feb 03, 2004 10:32 am

I have a couple pieces with a burr on the edge -- a little sharp bit that's very unappealing. Small enough that it seems a waste to grind and go through a whole fire-polishing cycle ... is this something that a diamond hand pad would clean up?

Thanks -- Marilyn

Ron Coleman
Posts: 468
Joined: Sun Mar 09, 2003 3:20 pm
Location: Columbus, Ohio USA

Postby Ron Coleman » Tue Feb 03, 2004 10:44 am

The diamond pads will work, but I find them hard to control on small edges. One slip and you scratch the surface of your piece.

For fine details I like to use diamond honing sticks.

http://shop.woodcraft.com/Woodcraft/pro ... D4637914AA

Ron

Marilyn Kaminski
Posts: 22
Joined: Wed Mar 12, 2003 10:27 am
Location: Boulder, CO

Postby Marilyn Kaminski » Tue Feb 03, 2004 10:50 am

Coarse, medium, fine, or superfine?

- M

Ron Coleman
Posts: 468
Joined: Sun Mar 09, 2003 3:20 pm
Location: Columbus, Ohio USA

Postby Ron Coleman » Tue Feb 03, 2004 10:56 am

Marilyn Kaminski wrote:Coarse, medium, fine, or superfine?

- M


I find the fine and superfine to be the most useful.

Ron


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 46 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron