Pat K.
Posts: 53
Joined: Thu Aug 04, 2005 12:33 pm
Location: Pittsburgh, PA

Dichro Slide

Postby Pat K. » Thu Jul 19, 2012 2:12 pm

Is dichro slide supposed to go under clear glass or fire hot? I put some on some rather bland pendants - on top. I only took it to fire polish - 1350. It looked funny to me as I was carefull applying it; it seemed some had come off the edges. I rubbed the top of one of the pieces and it came off on my hand. It didn't come with any directions; I did a search on here with no results. Anyone have any clues - I'd be grateful. Thanks.

Patty
Patty

It often shows a command of language to say nothing - author unkown.

Kevin Midgley
Posts: 713
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Dichro Slide

Postby Kevin Midgley » Thu Jul 19, 2012 2:34 pm

you get what you pay for.

Lynn g
Posts: 91
Joined: Sun Nov 02, 2003 1:36 am
Location: Clovis, CA

Re: Dichro Slide

Postby Lynn g » Thu Jul 19, 2012 7:11 pm

I checked the Glasshopper website (www.glasshopperpatterns.com). Their dichro slide instructions say it works well uncapped, and they recommend using your "usual fusing" schedule. I suspect it needs to be fired up into the fusing range rather than just a firepolish.
Lynn g
"Patriotism is not enough, I must have no hatred or bitterness towards anyone." - Dame Edith Cavell

Pat K.
Posts: 53
Joined: Thu Aug 04, 2005 12:33 pm
Location: Pittsburgh, PA

Re: Dichro Slide

Postby Pat K. » Fri Jul 20, 2012 9:33 am

Thanks Lynn - I appreciate your helpfulness. Patty
Patty



It often shows a command of language to say nothing - author unkown.

dawnsud
Posts: 42
Joined: Mon Aug 01, 2005 5:03 pm
Location: Cedaredge, Colorado

Re: Dichro Slide

Postby dawnsud » Fri Jul 20, 2012 11:36 am

Most of the manufacturers have very helpful tech support people. If you don't know the manufacturer, call your supplier and find out.
Take care.
Dawn

Brad Walker
Site Admin
Posts: 1349
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Dichro Slide

Postby Brad Walker » Fri Jul 20, 2012 12:55 pm

Lynn's right. If you want to use it uncapped, you'll need to fire high enough to get the slide to melt a bit into the piece. A full fuse works best.

Raphael Schnepf
Posts: 24
Joined: Sat Oct 14, 2006 11:31 pm
Location: Milwaukie Oregon
Contact:

Re: Dichro Slide

Postby Raphael Schnepf » Fri Jul 20, 2012 4:38 pm

My wife Margaret uses Dichroslide a lot and prefers the look under a thin layer of clear. She has sandwiched it between several layers. Just like dichro glass the look is different (brighter) under clear glass.

Raf

Raphael Schnepf
Posts: 24
Joined: Sat Oct 14, 2006 11:31 pm
Location: Milwaukie Oregon
Contact:

Re: Dichro Slide

Postby Raphael Schnepf » Fri Jul 20, 2012 4:42 pm

you get what you pay for.


By the way Kevin this stuff's not cheap. It has its uses and works in ways the would be impossible for dichro glass.

Raf


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 33 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com