Postby deerick » Wed Sep 12, 2012 4:34 pm

The artist used glass and flameworked stringers then fused. Can I use Glassline or glass enamel with A4? Also, Do I cap the bottom layer with clear and paint on top of the clear, will that make it a flat surface?

http://www.etsy.com/listing/103199546/d ... pe=gallery

I know this is probably so very simple, but that is why I like it. Thank you

Brad Walker
Site Admin
Posts: 1335
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: how do i do this

Postby Brad Walker » Wed Sep 12, 2012 5:07 pm

It is not a good idea, nor is it legal, to copy someone else's design. Better to come up with your own design.

It is possible to paint on a flat piece of glass with either Glassline or enamels mixed with a binder (A-14 is often used). You can paint on the top layer, the bottom layer, or both. Applied and fired properly, the enamels will be flat on the surface of the glass. Designs can also be fired flat when using stringers and frit; it's just a matter of how high they are fired in the kiln. But in either case, come up with your own design, and avoid copying someone else's design.

HEIDI in Wa. state
Posts: 10
Joined: Tue Jul 26, 2005 12:51 am
Location: Washington state

Re: how do i do this

Postby HEIDI in Wa. state » Wed Sep 12, 2012 8:35 pm

Brad Walker wrote:It is not a good idea, nor is it legal, to copy someone else's design. Better to come up with your own design.

Thanks Brad, it is not my design either, but, for some reason we need to remind people of this sometimes...
HEIDI --who is having someone copy her designs right now....

deerick
Posts: 11
Joined: Wed Mar 17, 2010 9:52 pm

Re: how do i do this

Postby deerick » Wed Sep 12, 2012 9:22 pm

I just wanted to make sure everyone knows I was just looking for information on technique with no intention of copying the design. I actually have a frog from a coloring book:). Thanks

HEIDI in Wa. state
Posts: 10
Joined: Tue Jul 26, 2005 12:51 am
Location: Washington state

Re: how do i do this

Postby HEIDI in Wa. state » Wed Sep 12, 2012 10:30 pm

I didn't mean my comment to suggest you were going to copy, my statement was more a general one. Sorry if I offended you, I truly didn't mean too.
HEIDI

Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: how do i do this

Postby Morganica » Thu Sep 13, 2012 2:30 am

You can manipulate stringer with a candleflame and a couple pairs of tweezers or needle nose pliers, so you can do at least thinner lines without special equipment. Once the components get thicker you need a hotter torch or a vitragraph kiln setup.

Or you can cut flat glass a bit thicker than you want it, and give it a good flat fuse firing. It takes a little practice, but you can get a torch work effect with that, and the bottom is already flat, which makes it a bit easier to get to the kiln.

Then you just arrange the components and tack fuse them to the flat blank.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)

deerick
Posts: 11
Joined: Wed Mar 17, 2010 9:52 pm

Re: how do i do this

Postby deerick » Thu Sep 13, 2012 9:38 am

No offense taken. And thank you for all your help. This board is so great in helping is newbies


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 23 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron