Location: Canada

Schedule needed for glass nuggets

Post by Vicki M »

Hi,

I want to make some glass nuggets from the scrap Sys 96 glass I have, I will be cutting it into 1/2" squares and fusing 2 squares together. I have never made them before and I have a new kiln it's a Paragon Fusion 8 with sentry controller. Can someone please give me a firing schedule that I could start off with, I am still trying to get used to this new kiln.

Thank you :)
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: Schedule needed for glass nuggets

Post by Brock »

Turn it on high until done.
Turn it off.
Vicki M
Posts: 38
Joined: Sat Aug 30, 2003 10:56 am
Location: Canada

Re: Schedule needed for glass nuggets

Post by Vicki M »

So in other words do I ramp up ASAP to around 1450 check and then turn off?
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: Schedule needed for glass nuggets

Post by Brock »

Vicki M wrote:So in other words do I ramp up ASAP to around 1450 check and then turn off?
Yeah, that's all there is to it.
Barry Kaiser
Posts: 307
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: Schedule needed for glass nuggets

Post by Barry Kaiser »

Vicki,
You may need to hold some at 1450.
Check to see if they are done, then turn off the kiln.

Barry
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: Schedule needed for glass nuggets

Post by Brock »

"I want to make some glass nuggets . . ."

"Turn it on high until done. Turn it off."

"So in other words do I ramp up ASAP to around 1450 check and then turn off?"

Get it Barry? . . . until done . . . check . . .
carol carson
Posts: 58
Joined: Sat Jul 30, 2005 6:25 pm
Location: Portland OR
Contact:

Re: Schedule needed for glass nuggets

Post by carol carson »

We need a "Like" button on this board.
Vicki M
Posts: 38
Joined: Sat Aug 30, 2003 10:56 am
Location: Canada

Re: Schedule needed for glass nuggets

Post by Vicki M »

Thanks so much everyone as they say you don't learn if you don't ask. Even for the simplest of things. Thank you again for taking the time to reply. :)