Kiln-acrylic paints-fire brick-devit

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Dione Roberts
Posts: 9
Joined: Mon Sep 08, 2003 10:36 pm

Kiln-acrylic paints-fire brick-devit

Post by Dione Roberts »

I ran across a discussion the other day about someone who has been firing with acrylic paints in their kiln for some time and now gets devit on much of their system 96 glass. I am wondering if it is possible to ruin your kiln brick or elements in some way with acrylic paints or something unusual like that which might cause a release of gasses that would cause devit in subsequent firings. My thought is if your kiln has been vented the answer would be no but I am not sure. This is just something that has my curiousity piqued! :)
Post Reply