Postby seachange » Sat Oct 13, 2012 6:55 pm

Hi,

I am making a series of bowls, many are slumped into either the classic bowl or the ball mold, medium size.

The gallery that is interested in these told me they would like rubber feet on them. They find many of their customers are concerned about scratching their furniture (either glass or wood surfaces).

Last year I bought some generic brand bumpons at the local hardware store, but they fall off eventually.

Has anyone got experience with this, could you please recommend a brand, and perhaps a good shape? Intend to use 3 on each bowl. I am thinking that as flat and as invisible as possible would be best, but not too small, otherwise there is not enough glue surface.

Many thanks, seachange

Michele gh
Posts: 71
Joined: Tue Sep 21, 2004 11:10 pm
Location: Massachusetts
Contact:

Re: best quality bump on feet for bowls

Postby Michele gh » Sat Oct 13, 2012 7:05 pm


Tom Fuhrman
Posts: 176
Joined: Mon Mar 10, 2003 11:44 am
Location: eastern Tennessee
Contact:

Re: best quality bump on feet for bowls

Postby Tom Fuhrman » Sat Oct 13, 2012 7:33 pm

just bought a couple thousand 3-M brand and they seem to be working very well. they were much cheaper than any others I found. can send you some if you need a few hundred. about $.06 ea. if any of them get very hot they can slip around and fall off. don't put them on a light or in intense sunlight where they can get hot.no matter who made them.

Lynn g
Posts: 91
Joined: Sun Nov 02, 2003 1:36 am
Location: Clovis, CA

Re: best quality bump on feet for bowls

Postby Lynn g » Sat Oct 13, 2012 11:30 pm

I got some nice and tiny bump-ons from His Glassworks (look under "acccessories")...current price shows as $4.95 for a sheet of 225. I've used them on coasters for a few years now, and they stick well and are unobtrusive. I really like them.
Lynn g
"Patriotism is not enough, I must have no hatred or bitterness towards anyone." - Dame Edith Cavell

seachange
Posts: 223
Joined: Tue Apr 18, 2006 1:19 am

Re: best quality bump on feet for bowls

Postby seachange » Sun Oct 14, 2012 2:49 am

Michele gh wrote:http://bumperspecialties.com/home-en.php


Thanks Michele, good to see a specialized company, and US made. I'll check quantities with them.

Best regards, seachange

seachange
Posts: 223
Joined: Tue Apr 18, 2006 1:19 am

Re: best quality bump on feet for bowls

Postby seachange » Sun Oct 14, 2012 2:55 am

Lynn g wrote:I got some nice and tiny bump-ons from His Glassworks (look under "acccessories")...current price shows as $4.95 for a sheet of 225. I've used them on coasters for a few years now, and they stick well and are unobtrusive. I really like them.


Thanks Lynn, I have to email His, because I remember trying to look at them before placing my order, but the bottom half of his accessories page does not open for me. By the time I had put together the rest of my order, forgot completely about the feet.

Many thanks, seachange

seachange
Posts: 223
Joined: Tue Apr 18, 2006 1:19 am

Re: best quality bump on feet for bowls

Postby seachange » Fri Oct 19, 2012 11:45 pm

Fuhrman Glass Studios Inc wrote:just bought a couple thousand 3-M brand and they seem to be working very well. they were much cheaper than any others I found. can send you some if you need a few hundred. about $.06 ea. if any of them get very hot they can slip around and fall off. don't put them on a light or in intense sunlight where they can get hot.no matter who made them.


Hi Tom, which ones did you get?

Many thanks for the offer, I have sent you a PM about the possibility of shipping some to me.

However, if I know the number of the ones you are happy with, I can first try to get them locally. 3M has an extensive list of different ones, and there is a distributor in Australia, but it does not mean they actually carry in stock everything that is in the catalogue.

Thanks again, best regards, seachange


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 16 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com