Postby Beau Lyons » Sun Oct 14, 2012 3:37 am

Have any of you guys used fused glass over stone chips.

Mark Hughes
Posts: 37
Joined: Mon Mar 17, 2003 6:27 pm
Location: Omaha, Nebraska

Re: fused glass and stone.

Postby Mark Hughes » Sun Oct 14, 2012 12:47 pm

I would think you would need stone with the same or very near the same COE as the glass to keep from fracturing.
Mark Hughes

Lynn g
Posts: 91
Joined: Sun Nov 02, 2003 1:36 am
Location: Clovis, CA

Re: fused glass and stone.

Postby Lynn g » Mon Oct 15, 2012 12:48 am

LOots in the archives, I believe. Try a search there.
Lynn g
"Patriotism is not enough, I must have no hatred or bitterness towards anyone." - Dame Edith Cavell

Beau Lyons
Posts: 32
Joined: Fri Sep 21, 2012 11:47 pm

Re: fused glass and stone.

Postby Beau Lyons » Sat Nov 24, 2012 3:27 am

Has anyone had experience with this,
I am not trying to fuse the stone, just the glass, over the stone.

rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: fused glass and stone.

Postby rosanna gusler » Sat Nov 24, 2012 8:40 am

Go to search at top of page. Type in glass rocks. Enjoy. Rosanna
artist, owner of wanchese art studio, marine finisher


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 27 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com