While shopping locally today I found a product labeled Maninite, by BNZ Materials. It is a calcium silicate structural material.
I am thinking this could work for daming and boxes for sand castings.
Has anyone had experience with this product"?
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Refractory product question

Post by Bert Weiss »

It is marinite. I would lean towards vermiculite boards as they hold together with stainless steel screws. I plan to use calcium silicate boards as backup insulation for kiln building. I tried Marinite as a kiln shelf for firing enameled stained glass. It warps though.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Marvin
Posts: 4
Joined: Wed Aug 10, 2011 11:12 pm

Re: Refractory product question

Post by Marvin »

Thanks for you input and spelling correction :)
I started out looking for fiberfrax, no luck.
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Refractory product question

Post by Bert Weiss »

Marvin wrote:Thanks for you input and spelling correction :)
I started out looking for fiberfrax, no luck.
Unifrax makes Durablanket which is what people call fiberfrax. They also make Duraboards HD and LD these are rated for higher temperatures than calcium silicate boards. HD stands for high density, LD low density.

Vermiculite boards come in different densities as well. The more dense are stronger and less insulating.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Refractory product question

Post by twin vision glass »

Where abouts are you Marvin. http://www.zrci.com is a wonderful place and likes to help out the glass artists. Hmm eh! :-k
P.S. they even have a section for glass artists down on the left bottom. Just click on that section Les
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
Keoni
Posts: 13
Joined: Sat Mar 19, 2005 1:58 am
Location: Vancouver, Wa

Re: Refractory product question

Post by Keoni »

Marinite has a tendancy to warp. Cut up mullite kiln shelves work very well, you can also cast your own dams out of products such as Greenlite 45.