Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

school project

Postby Laurie Spray » Tue Dec 11, 2012 4:12 pm

I am helping with a fundraiser for a local school. The kiddos are each going to make 2" tiles that will be assembled at school and transported to our studio and fired into a platter. Question.....the only glue I have ever used in my own work is super glue....which is not good for kids to use. If they just use an elmers white glue will it all burn off? Knowing kids they will use more then they need.....could get messy. I am sure this may have all been discussed but I was looking for a quick comment or two.
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com

AndyT
Posts: 150
Joined: Mon Apr 30, 2007 9:34 am
Location: Medford, Orygun
Contact:

Re: school project

Postby AndyT » Tue Dec 11, 2012 5:44 pm

I've used Elmers and Weldbond. Just a very small dab is all you need. Usually a dab the size of a pin head is enough.

bob proulx
Posts: 186
Joined: Tue Dec 29, 2009 7:13 pm
Location: Nahant Massachusetts
Contact:

Re: school project

Postby bob proulx » Tue Dec 11, 2012 6:25 pm

You may not want to use this with the kids but a hot glue gun works great, A little dab will do you. :D
Bob

dawnsud
Posts: 42
Joined: Mon Aug 01, 2005 5:03 pm
Location: Cedaredge, Colorado

Re: school project

Postby dawnsud » Tue Dec 11, 2012 7:14 pm

Keep the Elmer's near the edge of the piece or it won't burn off. But the edge is about 1/4 inch.
Take care.
Dawn

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: school project

Postby Valerie Adams » Tue Dec 11, 2012 9:05 pm

You could also have them use cheap non-aerosol hairspray. I keep it in a little bottle with a narrow pointed tip.

Studiodunn
Posts: 106
Joined: Sun Sep 11, 2011 9:30 am
Location: The Dunn-Inn
Contact:

Re: school project

Postby Studiodunn » Wed Dec 12, 2012 12:08 am

What Valerie said...El cheapo, White Rain, unscented hair spray in a little "plastic oil dispenser" with a fine metal tip. Works like a charm!
“I would rather die than hate you.”
- Martin Luther King

Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: school project

Postby Laurie Spray » Wed Dec 12, 2012 12:20 am

Of course!! Hair spray!! Thanks guys! Happy holidays!
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com

Kevin Midgley
Posts: 713
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: school project

Postby Kevin Midgley » Wed Dec 12, 2012 3:17 am

hair spray smells. somebody in a class is bound to be chemically sensitive.
white glue in small open container and a box of toothpicks telling everyone to keep their hands really really clean
Make laser printer decals of all the kid's names. Get list in advance of class and make decals.
soak and slide decal on the base. kids love doing that.
Let any kids who finish fast make one for the absentee kids.
If you don't use decals, nobody can remember what they made.

Jamiefran
Posts: 1
Joined: Fri Jan 30, 2009 12:15 am

Re: school project

Postby Jamiefran » Thu Dec 13, 2012 4:11 pm

My main glass work is with kids for school auctions. We use(and reuse) paper plates with kids names and take a digital picture of each to keep track of whom did what. I use elmer's blue school glue with toothpicks. While I have not had many issues typically, I did notice some darkened smoky looking areas when I used that glue, BE French Vanilla and a small piece of copper sandwiched between clear and BE French Vanilla.

Next time I'll try the hairspray. How do you transport your glass works from school to kiln with the hairspray? Does it hold like glue?

Jamie

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: school project

Postby Valerie Adams » Thu Dec 13, 2012 4:25 pm

Hairspray holds really well. I use unscented White Rain or Rave non-aerosol hairspray from the dollar store.
If you're already putting the kids' work on paper plates, you could just cover them with saran wrap and gently stack. The hairspray will hold just fine, and I've never had any issues with residue or smell.

dawnsud
Posts: 42
Joined: Mon Aug 01, 2005 5:03 pm
Location: Cedaredge, Colorado

Re: school project

Postby dawnsud » Thu Dec 13, 2012 5:25 pm

Great idea, Valerie. I've worried about transporting the work to the kiln. Even looked into buying a fiber kiln but opted out on that.
Take care.

Dawn

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: school project

Postby Valerie Adams » Thu Dec 13, 2012 6:06 pm

dawnsud wrote:Great idea, Valerie. I've worried about transporting the work to the kiln. Even looked into buying a fiber kiln but opted out on that.


I've got a couple of the fiber kilns, which I originally bought for travel-teaching. But while they're lighter than brick kilns, they're not exactly light enough to tote around. The BonnieGlo is fairly easy to manage but the 16" square fiber kilns are too large to move alone. I also had my neck rebuilt in April, so carrying kilns around is not in my immediate future!

S.TImmerman
Posts: 235
Joined: Wed Nov 25, 2009 9:23 am
Location: San Diego ,Ca

Re: school project

Postby S.TImmerman » Fri Dec 14, 2012 6:02 am

Kevin Midgley wrote:hair spray smells. somebody in a class is bound to be chemically sensitive.
white glue in small open container and a box of toothpicks telling everyone to keep their hands really really clean
Make laser printer decals of all the kid's names. Get list in advance of class and make decals.
soak and slide decal on the base. kids love doing that.
Let any kids who finish fast make one for the absentee kids.
If you don't use decals, nobody can remember what they made.



Laura , if you'd like to do that and don't have the printer/decals. I'm happy to help you, email me the names and I'll mail you the decals - :)


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 41 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com