flite risk
Posts: 2
Joined: Sat Mar 04, 2006 10:54 am
Location: Hamilton, MT

MICR Printer owners

Postby flite risk » Sun Dec 23, 2012 1:15 pm

I have been looking at MICR printers lately and have searched the archives for any information on them. It has been a bit confusing because most of them have become obsolete and when I try and research the current printers listed I find that they don't mention that they are MICR capable. It would be great to hear from folks that do have one of these current printers and where they purchased it. I really like the sepia images and want to start making them.

Thanks!
Tom
SDG

Brad Walker
Site Admin
Posts: 1372
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: MICR Printer owners

Postby Brad Walker » Sun Dec 23, 2012 7:23 pm

flite risk wrote:I have been looking at MICR printers lately and have searched the archives for any information on them. It has been a bit confusing because most of them have become obsolete and when I try and research the current printers listed I find that they don't mention that they are MICR capable. It would be great to hear from folks that do have one of these current printers and where they purchased it. I really like the sepia images and want to start making them.


I assume you want to print decals. MICR is not a type of printer. It is a type of toner that is used to print checks. You can get MICR toner for most laser printers. However, don't make the mistake of thinking that if you have MICR toner you can print decals. That's not necessarily the case.

Instead, look for a printer that can use a toner with a relatively high iron content. Most HP laser printers fit into this category. You'll have to use the HP brand toner; many of the off brand toners won't work.

Barry Kaiser
Posts: 290
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: MICR Printer owners

Postby Barry Kaiser » Sun Dec 23, 2012 8:23 pm

Gotta disagree with you Brad. I've used off brands for several different HP (6P, 1020, 1018) printers and they all work fine.
I believe the printing process for HPs is magnetic and need the iron in the toner to work...thus the no-names work fine.

Barry

Brad Walker
Site Admin
Posts: 1372
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: MICR Printer owners

Postby Brad Walker » Sun Dec 23, 2012 11:50 pm

Barry Kaiser wrote:Gotta disagree with you Brad. I've used off brands for several different HP (6P, 1020, 1018) printers and they all work fine.
I believe the printing process for HPs is magnetic and need the iron in the toner to work...thus the no-names work fine.


They don't all work, Barry. Perhaps most do, but they certainly don't all work. We've had off brands that work and off brands that didn't.

GlassCat
Posts: 24
Joined: Thu May 06, 2010 5:46 pm

Re: MICR Printer owners

Postby GlassCat » Mon Dec 24, 2012 12:15 am

I have an HP P1006 which is one of the lowest prices HP carries and it prints decals just fine but I do use the HP brand toner cartridge--have tried the recycled ones and didn't work for me.

Carol

bob proulx
Posts: 186
Joined: Tue Dec 29, 2009 7:13 pm
Location: Nahant Massachusetts
Contact:

Re: MICR Printer owners

Postby bob proulx » Mon Dec 24, 2012 9:32 am

I also have the hp p 1006 and it works well I don't think they make this model any more but they have something new in the same price range. Check out the HP store on line, I paid $99.00 with free shipping.
Bob

flite risk
Posts: 2
Joined: Sat Mar 04, 2006 10:54 am
Location: Hamilton, MT

Re: MICR Printer owners

Postby flite risk » Mon Dec 24, 2012 2:02 pm

Thanks all for the input!

Brad, I understand now that it requires the magnetic transfer for the iron content in the toner. thanks!

Based on the feedback from you folks I went to the HP site and found what I think is the closest replacement to the P1006 which is the HP LaserJet Pro P1102w Printer. They want $130 for it which seems cheap to me but I think is what I need.

I also found the HP MSDS library: http://www.hp.com/hpinfo/globalcitizens ... useng.html

The MSDS for the P1102w cartridge (CE285A) shows that it has <45 ferrite which I am hoping is enough for the decals. It does not say what the exact content is but it also shows that it ships as a magnetized material so I am assuming that is good. I also checked online for off brand cartridge suppliers and they supply a micr cartridge for this model which also bodes well. So unless I hear differently, I think I will go ahead and get this model.

I am looking forward to printing some decals. I see quite a few decal suppliers but it looks like the manufacturer might be the same.

Thanks for your replies!

Tom
SDG

Mike Griffin
Posts: 23
Joined: Mon Apr 01, 2013 10:04 pm
Location: Gelorup, Western Australia

Re: MICR Printer owners

Postby Mike Griffin » Tue Apr 02, 2013 6:52 am

I've just bought a P1102w printer and it works great. I couldn't believe that it only cost $89. The standard toner #85, CE285A has >45% iron pigment and it produces great sepia fused glass prints. No need to search for a MICR toner cartridge.

JestersBaubles
Posts: 698
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: MICR Printer owners

Postby JestersBaubles » Tue Apr 02, 2013 1:40 pm

My husband just purchased a Canon laser printer, I think the MF4880. I checked the MSDS on the toner cartridge, and it has fairly high iron (ferrite) content. I am going to give it a try in a few weeks using gel medium (I'll be traveling through April 20, so no time for glass for a while after the expo). I'll report back on how it goes.

Dana W.

bob proulx
Posts: 186
Joined: Tue Dec 29, 2009 7:13 pm
Location: Nahant Massachusetts
Contact:

Re: MICR Printer owners

Postby bob proulx » Tue Apr 02, 2013 2:21 pm

JestersBaubles wrote:My husband just purchased a Canon laser printer, I think the MF4880. I checked the MSDS on the toner cartridge, and it has fairly high iron (ferrite) content. I am going to give it a try in a few weeks using gel medium (I'll be traveling through April 20, so no time for glass for a while after the expo). I'll report back on how it goes.

Dana W.

Hi Dana, what do you mean by gel medium.
Bob

LDGlass
Posts: 22
Joined: Sun Mar 23, 2003 2:54 pm
Location: Milwaukee, WI
Contact:

Re: MICR Printer owners

Postby LDGlass » Tue Apr 02, 2013 2:52 pm

I went online (Amazon.com I think) and just ordered a micr toner for my printer (Samsung) and it works great for decals.

JestersBaubles
Posts: 698
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: MICR Printer owners

Postby JestersBaubles » Tue Apr 02, 2013 9:21 pm

bob proulx wrote:Hi Dana, what do you mean by gel medium.
Bob


I haven't tried it yet but supposedly...

Print your image on a laser printer with high iron content. Paint the printed image with matte gel medium (painters use it to thin paints), place on irid glass and fire. Image is transferred to the glass.

Cheaper than photo paper or decals :mrgreen:, though if IIRC, it does have to be irid glass for the image to transfer and "stick", and I believe it's recommended that you cap it later. I need to pull out my notes.

Dana W.

Mike Griffin
Posts: 23
Joined: Mon Apr 01, 2013 10:04 pm
Location: Gelorup, Western Australia

Re: MICR Printer owners

Postby Mike Griffin » Thu Apr 04, 2013 1:29 am

Similar to what I'm doing. Laser print on plain paper. Thin layer of artist's acrylic varnish (eg. Aleen's Enhancers gloss varnish but others work too) on glass and stick paper print side down to wet surface avoiding bubbles. I'm not using iridised glass. Paper burns off at about 450 deg C in a slumping cycle leaving a fine ash, some of which makes the glass surface hazy but most of the image adheres. When capped and full fused the haziness disappears, supposedly it dissolves in the glass. Inspected with crossed polarisers there is no sign of stress at the joint. I haven't yet found an ashless paper that doesn't lift or buckle at the ashing stage.

bob proulx
Posts: 186
Joined: Tue Dec 29, 2009 7:13 pm
Location: Nahant Massachusetts
Contact:

Re: MICR Printer owners

Postby bob proulx » Thu Apr 04, 2013 5:49 am

Thanks Dana and Mike.
Bob


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 70 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com