Postby daffodildeb » Fri Feb 06, 2004 4:11 am

I can't for the life of me melt 1 and 2mm BE stringers. I've heard you can use a candle--didn't work. I have a Hothead torch, but I suspect that's overkill to say the least.

All I want is little squigglies! Ideas?

:-k
Deb

Diane
Posts: 56
Joined: Sun Mar 09, 2003 3:59 pm
Location: Kennebunkport, Maine

Postby Diane » Fri Feb 06, 2004 4:46 am

I just hold them IN a candle flame and they start to soften very quickly. It seems to only heat up a small section so you need to work your way down the stringer, bending and twisting as you go. It takes some practice but fun to do.
Good Luck, Diane

daffodildeb
Posts: 125
Joined: Mon Jul 28, 2003 3:48 am
Location: Hot Springs Village, AR

Postby daffodildeb » Fri Feb 06, 2004 5:18 am

Thanks--I'll give it a try--no soot?
Deb

Mike Byers
Posts: 56
Joined: Mon Mar 10, 2003 6:57 pm
Location: west central Indiana
Contact:

Postby Mike Byers » Fri Feb 06, 2004 6:47 am

Yes, you'll get soot: that's the disadvantage of using a candle. A regular propane torch is a lot cleaner: just hold the stringer above the flame to keep it from melting too quickly.

Peg
Posts: 74
Joined: Tue Apr 08, 2003 7:50 am
Location: Bristol, UK

Postby Peg » Fri Feb 06, 2004 8:14 am

I use the gas flame of my kitchen hob to work stringer. I even bend rod that way, a bit.
Candles are fine but very sooty - the gas flame is soot free.
I am assuming gas cookers are not just a European thing...

Michael McNerney
Posts: 41
Joined: Tue Mar 18, 2003 12:22 pm
Location: Hilliard, Ohio

Postby Michael McNerney » Fri Feb 06, 2004 8:37 am

daffodildeb,
I also usually use a tea ight candle, Yes I do get soot. the soot will burn off during your fire. I do this with dichroic stringers all of the time and haven't had a problem yet.

you can also go to the hardware store and buy a small plumbing torch if you dont want to invest into a lamp working torch.

vblue
Posts: 98
Joined: Sun Mar 09, 2003 11:05 pm
Location: Texas

Postby vblue » Fri Feb 06, 2004 10:22 am

Any candle will do. I find that the tea candles work better. You have to hold the stringer in the flame for about 4-5 seconds, apply gentle pressure and the stringer will bend. I've also bent noodles.
Sometimes using the pointy tweezers help in bending shapes.
You do get soot but it does burn off.
I couldn't get the image thingy to work, but click on the link below and see photo.

Vernelle

http://pic2.picturetrail.com/VOL29/4003 ... 822492.jpg

Goldfinger
Posts: 54
Joined: Wed Jan 07, 2004 11:07 am
Location: Missouri

Melting Stringers

Postby Goldfinger » Fri Feb 06, 2004 11:13 am

If you want a clean flame- do a Google search on "Alcohol Burners". This should lead you to a labratory supply website. They are relatively inexpensive. It's been so long since I've used one I can't recall what type of alcohol I used. You might be able to get by with the common rubbing alcohol you find in the drugstore. Check with your supplier.

Steve

Gordon Exon
Posts: 5
Joined: Mon Feb 02, 2004 8:22 pm
Location: Calgary

Alcohol lamps

Postby Gordon Exon » Fri Feb 06, 2004 11:58 am

jewellers supply sometimes have them. The alcohol is methyl hydrate and I've found the best way to get it in small quantities is to do to the gas station and buy a small bottle of gas line anti freeze, same stuff

starchimes (Andrea)
Posts: 26
Joined: Tue May 20, 2003 11:39 am
Location: Dallas, TX
Contact:

Postby starchimes (Andrea) » Fri Feb 06, 2004 12:20 pm

I use a bic lighter. If the flame goes, it can get really hot trying to restrike the lighter, but it works like a charm.

JJ
Posts: 11
Joined: Tue Sep 09, 2003 8:16 am
Location: North Carolina

Postby JJ » Fri Feb 06, 2004 1:48 pm

I use an oil candle- you know the kind that you fill with 99% liquid wax paraffin. I don't get any soot on the stringers by using this and holding just slightly above the flame-twisting and turning as it melts. You can get some tight squiggles if you start to turn just as it starts to bend.
JJ in NC

Diane Trepanier
Posts: 17
Joined: Mon Aug 11, 2003 9:54 pm
Location: Maryland

Postby Diane Trepanier » Fri Feb 06, 2004 3:47 pm

Another option to consider is a small butane micro torch. I picked one up at Costco (I have seen them in hardware stores, etc.) for $20. Uses butane lighter fluid and will run for about 1 -1 1/2 hrs depending on how you adjust the flame. Will sit on it's on stand. Fast, easy, quick!
Diane Trepanier
Solfyre
Designer, glass, wire, beads, etc.

daffodildeb
Posts: 125
Joined: Mon Jul 28, 2003 3:48 am
Location: Hot Springs Village, AR

Postby daffodildeb » Fri Feb 06, 2004 5:06 pm

Thanks, all! I've been practicing with a candle, and getting what I want, except for the soot. I'll try my gas stove (it may be the only way it will redeem itself because I hate cooking with gas!), or perhaps an oil candle. I have both.
Deb

Barbara Muth
Posts: 382
Joined: Sun Mar 09, 2003 8:10 pm
Location: Washington DC Metropolitan Area
Contact:

Postby Barbara Muth » Fri Feb 06, 2004 8:47 pm

Deb I just fire the stringers on top of a piece, soot and all. The soot has never left a trace for me.

Barbara
Barbara
Check out the glass manufacturer's recommended firing schedules...
LATEST GLASS

Diane
Posts: 56
Joined: Sun Mar 09, 2003 3:59 pm
Location: Kennebunkport, Maine

Postby Diane » Sat Feb 07, 2004 5:02 am

I just fire the stringers on top of a piece, soot and all. The soot has never left a trace for me.

ME TOO
Squiggle n' go

Alecia Helton
Posts: 108
Joined: Mon Aug 25, 2003 12:35 am
Location: outside of Dallas TX

Postby Alecia Helton » Sat Feb 07, 2004 11:07 am

The soot rinses off under running water then you don't get it all over your fingers.

Alecia
Alecia Helton
Wear Original Wonders!
Carrollton TX


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: Google [Bot] and 20 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com