using pizza stone? for fusing on

Postby bothofushk » Wed Jan 23, 2013 11:42 am

Hi all,,I have never used one,,but I am thinking I would still have to KW or use thinfire on it,,right?

bothofushk

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: using pizza stone? for fusing on

Postby Valerie Adams » Wed Jan 23, 2013 12:06 pm

I use them all the time! I pick them up for a buck or so a garage sales or thrift stores, cook them to just above full-fuse temp before using them (they're usually filthy), then kiln wash. I've had a few break if I ramp too fast but for the most part, they're just kiln shelves.

Bert Weiss
Posts: 2338
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: using pizza stone? for fusing on

Postby Bert Weiss » Wed Jan 23, 2013 12:26 pm

I once visited a factory that makes mullite kiln shelves and furniture. Sitting next to all those was the pile of pizza stones. They are identical to kiln shelves, and require the same separator to prevent sticking.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

bob proulx
Posts: 186
Joined: Tue Dec 29, 2009 7:13 pm
Location: Nahant Massachusetts
Contact:

Re: using pizza stone? for fusing on

Postby bob proulx » Wed Jan 23, 2013 1:12 pm

I also use them all the time. I have 2 I have been using for over 5 years, their still going strong.
Bob

bothofushk
Posts: 42
Joined: Sat Jan 22, 2005 3:10 pm
Location: East Texas

Re: using pizza stone? for fusing on

Postby bothofushk » Thu Jan 24, 2013 9:19 am

thanks everyone,,,

bothofushk

Georgia Novak
Posts: 28
Joined: Wed Jun 04, 2003 2:54 am

Re: using pizza stone? for fusing on

Postby Georgia Novak » Fri Jan 25, 2013 7:33 pm

The one I have is only about 1/2 as thick as my regular kiln shelves. Is this normal? Do I need to ramp up more slowly? Georgia

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: using pizza stone? for fusing on

Postby Valerie Adams » Fri Jan 25, 2013 9:53 pm

My pizza stones are thinner than my kiln shelves, too. I don't ramp faster than 400°on them now as I did break a few by ramping at 600°an hour.

Georgia Novak
Posts: 28
Joined: Wed Jun 04, 2003 2:54 am

Re: using pizza stone? for fusing on

Postby Georgia Novak » Sun Jan 27, 2013 4:47 pm

Thanks Valerie. I have been afraid to use the pizza stone because of the thickness. Georgia

Bert Weiss
Posts: 2338
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: using pizza stone? for fusing on

Postby Bert Weiss » Sun Jan 27, 2013 8:24 pm

My common sense says that a thinner shelf would be less prone to heat shock, not more prone, just like glass...

I don't mean to contradict Valerie at all though. In her kiln 400dph may well be a good rate to ramp up. All kilns are not the same relative to this sort of thing.
Bert



Bert Weiss Art Glass*

http://www.customartglass.com

Furniture Lighting Sculpture Tableware

Architectural Commissions


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 60 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com