Penny Wise and Pound Foolish

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
sbaddley
Posts: 11
Joined: Sun Mar 09, 2003 8:53 pm
Location: Smithfield, Ut

Penny Wise and Pound Foolish

Post by sbaddley »

Was working on a project using my Taurus Ring Saw and the blade broke. After changing the blade, a series of cuts that took a lot of pressure on the blade and about 5 minutes now takes less than a minute and very little pressure on the blade. Who Knew? Guess I should think about changing my grinder head.

Every once in a while I have to call myself out for being too cheap and foolish. :D
Scott B
Nicole Hanna
Posts: 27
Joined: Wed Jul 27, 2005 10:17 am
Location: SW Missouri
Contact:

Re: Penny Wise and Pound Foolish

Post by Nicole Hanna »

I do the same thing, but those blades are so darn expensive ya just hate to not use it till it finally screams and breaks on ya!

Nicole
When I stand before God at the end of my life, I would hope that I would have not a single bit of talent left and could say, "I used everything you gave me." (erma bombeck)
Post Reply