PDXBarbara
Posts: 292
Joined: Sun Mar 09, 2003 4:09 pm
Location: Portland, OR

belts

Postby PDXBarbara » Thu Feb 28, 2013 5:12 pm

Fave cost-effective places to buy silicone carbide belts, 4 x 106?

The Oregon co, Sattex, I used to order from when I shared a belt-sander-equipped studio has dropped its abrasives line. As I recall, their prices were pretty reasonable.

HIS is something like $45 for a box of five 60-grits ($9/each). Grainger has boxes of 25 for like $695 (only looked at 120 grit) which is about $28/belt. Is CRL cheaper? (they won't give me prices without getting at least a DBA.) Yowza. Thanks.
Last edited by PDXBarbara on Thu Feb 28, 2013 5:20 pm, edited 1 time in total.
Barbara Bader

Marty
Posts: 852
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: belts

Postby Marty » Thu Feb 28, 2013 5:19 pm

HIS requires a dba? you sure?
I found HIS a little more expensive than CRL but much nicer to deal with and worthy of the support.
You could also befriend a local auto/window glass shop and see if they'll "share".

PDXBarbara
Posts: 292
Joined: Sun Mar 09, 2003 4:09 pm
Location: Portland, OR

Re: belts

Postby PDXBarbara » Thu Feb 28, 2013 5:21 pm

noooo. I'd written those sentences out of order. I just edited the damn thing. I'd hoped to catch it before inquiring & famous minds saw it.
Barbara Bader

Bert Weiss
Posts: 2337
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: belts

Postby Bert Weiss » Thu Feb 28, 2013 6:09 pm

PDXBarbara wrote:Fave cost-effective places to buy silicone carbide belts, 4 x 106?

The Oregon co, Sattex, I used to order from when I shared a belt-sander-equipped studio has dropped its abrasives line. As I recall, their prices were pretty reasonable.

HIS is something like $45 for a box of five 60-grits ($9/each). Grainger has boxes of 25 for like $695 (only looked at 120 grit) which is about $28/belt. Is CRL cheaper? (they won't give me prices without getting at least a DBA.) Yowza. Thanks.
CRL charges me $39.12 for a box of 5 - 120 grit belts (or 220,400). The price drops to $35.85 for 5 boxes. The grits are mixable for the discount.

80x costs $41.41, cork belts are $54.72 each, and the rest are $39.12

You must have some bud in the G guild who has an account at CRL.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Re: belts

Postby Tony Smith » Thu Feb 28, 2013 7:40 pm

Just go in and tell the salesman that you're a glass artist, that you have a CRLaurence wet belt sander and you want an account so you can buy belts. That's how I got my CRL account.

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun

S.TImmerman
Posts: 235
Joined: Wed Nov 25, 2009 9:23 am
Location: San Diego ,Ca

Re: belts

Postby S.TImmerman » Thu Feb 28, 2013 7:54 pm

I check eBay periodically and just bought cl belts (3 boxes of 5) 120 grit for 60.00. I should mention these are NOT from cl account on eBay. But rather an individual who is getting out of glass work. Last week I bought two boxes of 5 (80 grit) from another seller for 34.00. eBay as well as PayPal have excellent buyer protection help if needed. I have had to use it in the past once was paid back in 3 days.

Kevin Midgley
Posts: 713
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: belts

Postby Kevin Midgley » Thu Feb 28, 2013 8:39 pm

Check this one out but you'd have to enquire to get wholesale pricing
http://www.hitechglazing.com/product/43202/40382

PDXBarbara
Posts: 292
Joined: Sun Mar 09, 2003 4:09 pm
Location: Portland, OR

Re: belts

Postby PDXBarbara » Fri Mar 01, 2013 5:44 pm

Good suggestions, guys. Thanks.
Barbara Bader

Jerrwel
Posts: 129
Joined: Thu Feb 10, 2005 6:25 pm
Location: Charlotte, NC

Re: belts

Postby Jerrwel » Mon Mar 11, 2013 5:02 pm

I bought mixed-grit assortment of belts from Covingtonhttp://www.covington-engineering.com/index.html recently; great experience and the prices seemed reasonable.
Jerry

Doug Randall
Posts: 102
Joined: Sun Aug 17, 2003 10:11 pm
Location: Portland, OR
Contact:

Re: belts

Postby Doug Randall » Mon Mar 11, 2013 6:12 pm

Barbara. Call me, I've got belts you might be interested in.
Last edited by Doug Randall on Mon Mar 11, 2013 8:28 pm, edited 1 time in total.

Bert Weiss
Posts: 2337
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: belts

Postby Bert Weiss » Mon Mar 11, 2013 6:21 pm

Doug Randall wrote:Try here: http://www.abrasivesales.com/prodmenu.asp

Good prices and service. (80 grit) 4x106 SiCa belts run about $12.30 each when you buy a dozen.

The CRL price of $41.41 is for a box of 5 - 4x106 - 80 grit A discount down to $37.93 is for 5 boxes, mix and match.
Bert



Bert Weiss Art Glass*

http://www.customartglass.com

Furniture Lighting Sculpture Tableware

Architectural Commissions

jim simmons
Posts: 454
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: belts

Postby jim simmons » Tue Mar 12, 2013 4:36 pm

Me 2
Jim


Tony Smith wrote:Just go in and tell the salesman that you're a glass artist, that you have a CRLaurence wet belt sander and you want an account so you can buy belts. That's how I got my CRL account.

Tony


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 22 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com