Postby Jeanne » Mon Apr 01, 2013 8:35 pm

I am going to look at a used Somaca WBS (106G-RP24). I know very little about them (have only operated a WBS once) and would appreciate any input/tips as to what I should look at on the machine to ensure that it's in relatively good shape (or not).

Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: Used Wet Belt Sander Advice

Postby Brock » Mon Apr 01, 2013 8:49 pm

Check to see if the wheels have crowned. Turn it on, listen for ominous sounds.

Tom Fuhrman
Posts: 175
Joined: Mon Mar 10, 2003 11:44 am
Location: eastern Tennessee
Contact:

Re: Used Wet Belt Sander Advice

Postby Tom Fuhrman » Mon Apr 01, 2013 9:19 pm

bearings, platens, and other part that wear can be replaced fairly easily and are still availble even for very old ones. check to see that when tension is put on it that it runs fairly true.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: Google [Bot] and 54 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com