I used to put copper pennies in bottles and paperweights when I had my furnace. I would make a small indentation/cup in the gather then insert the coin and attach a 2nd gather on the cup's edge to encapsulate the coin. For fusers I would try making a small cup shape and then put the copper penny in and tack fuse a flat disc on the cup. Copper pennies are those that are classified as
wheat" pennies. I just found a jar with several hundred in a box I had stored and forgot I had.
Putting a coin in a small bottle shape on a torch should be quite easy. Seal off a tube, insert coin , seal other end tubing. Solid copper coins seem to work best just as inclusions of copper wire are easy to do.
making cabochon with coin inclusion?
Moderators: Brad Walker, Tony Smith
-
- Posts: 187
- Joined: Mon Mar 10, 2003 11:44 am
- Location: eastern Tennessee
- Contact:
-
- Site Admin
- Posts: 1489
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: making cabochon with coin inclusion?
Don't try this with pennies made after 1983 -- they're zinc, not copper. Pennies made before 1983 are copper, and pennies made in 1983 could be either.