Powder frit to hide devit?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Jeanne
Posts: 75
Joined: Wed Aug 20, 2003 8:16 am
Location: NJ

Powder frit to hide devit?

Post by Jeanne »

I have a 11" square pattern melt that I had sandblasted with aluminum oxide and refired to eliminate some devit. Well the devit remained on the BE Teal opal sections. If I sift 08 clear powder frit over the entire surface and refire, will it mask the devit?
Brad Walker
Site Admin
Posts: 1540
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Powder frit to hide devit?

Post by Brad Walker »

Yes. Just sift it in a very THIN layer, over all of the piece. Fire to full fuse.