Bullseye fiber paper causing opaque glass to be Matt

Postby helenrudy » Wed May 08, 2013 6:49 pm

I am making some pieces where the base glass is opaque bullseye color, red, blue etc. and it is fired directly onto the fiber paper On the shelf. The opaque glass where it is fired onto the paper is losing its sheen and is Matt and almost has a dusty appearance. Does anyone know why.
Any thoughts on what is causing this and how to prevent it.
Helen

Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: Bullseye fiber paper causing opaque glass to be Matt

Postby Brock » Wed May 08, 2013 7:00 pm

Prevent it by using kiln wash. Cheaper and effective.

helenrudy
Posts: 11
Joined: Mon Mar 08, 2010 11:31 pm

Re: Bullseye fiber paper causing opaque glass to be Matt

Postby helenrudy » Wed May 08, 2013 8:07 pm

I have been lazy with the paper. I hate it when the opaque glass sometimes stick to shelf and leaves a dent.

Jeanne
Posts: 75
Joined: Wed Aug 20, 2003 8:16 am
Location: NJ

Re: Bullseye fiber paper causing opaque glass to be Matt

Postby Jeanne » Wed May 08, 2013 8:29 pm

Are you venting the kiln to 1000 degrees?

Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: Bullseye fiber paper causing opaque glass to be Matt

Postby Laurie Spray » Wed May 08, 2013 8:39 pm

How hot are you firing?
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Bullseye fiber paper causing opaque glass to be Matt

Postby Valerie Adams » Thu May 09, 2013 8:58 am

Are you expecting your base sheet of opal glass to remain glossy on the bottom? That's not going to happen whether you use shelf paper or shelf wash. The bottom of your piece, during a full-fuse process, will pick up the texture of whatever you're firing it on.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 70 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com