I know you get what you pay for, BUT I was wondering if anyone had any recommendations on starter carving wheels for battuto. Something a novice like myself can cut their teeth on (no pun intended) with reasonable results and without spending $600.00 on a sintered diamond wheel at His Glass
I was thinking starting with a 325 grit and moving up. Should I go with diamonds or the poly resin bonded stuff. or the VID ones inbetween.

Any thoughts

Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Re: Carving wheels

Postby Tony Smith » Tue Jul 09, 2013 8:15 pm

Take a look at the lapidary wheels that Kingsley North carries. They carry 4" diameter x 1" thick radius wheels that work very well. www.kingsleynorth.com

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun

helenrudy
Posts: 11
Joined: Mon Mar 08, 2010 11:31 pm

Re: Carving wheels

Postby helenrudy » Tue Jul 09, 2013 8:30 pm

Thanks I will. H

Barbel
Posts: 17
Joined: Sat Dec 10, 2011 11:09 pm
Location: Ocean- Newport, North Carolina

Re: Carving wheels

Postby Barbel » Wed Jul 10, 2013 12:25 pm

I recently bought some wheels from Brad,

http://www.warmglass.org/servlet/the-Wh ... Categories
have not had a chance to try them yet, still setting up my new 'Baby Denver' ---Denver SAG1--- but used Brad's wheels in his studio and was happy with them,
also bought a couple of carving wheels from Denver (Brad did not have those in stock ). Their electroplated wheels were more reasonable than most sources.
Please share with us what you find with regards to sources and prices.
Have fun and hope you are as excited as I am to be playng with the lathe!
Barbel


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 48 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron