HP Cartridges that work for image transfer

Postby Brad Walker » Mon Aug 19, 2013 8:45 am

Jody Danner Walker's book "Printmaking Techniques on Glass" (more info here: http://www.warmglass.com/printmaking) lists several HP cartridges that can be used for photo transfer. The numbers cited in the book are:

12A
35A
36A
53A

Since the book was published, HP has added several cartridges to the line. If you know of any that work for photo transfer, please add them to this thread so that others can benefit.

(Please cite cartridge numbers, not printer models -- those come and go, the cartridges stay around longer and are used in multiple printers.)

Kevin Midgley
Posts: 686
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: HP Cartridges that work for image transfer

Postby Kevin Midgley » Mon Aug 19, 2013 12:10 pm

10A

JestersBaubles
Posts: 687
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: HP Cartridges that work for image transfer

Postby JestersBaubles » Mon Aug 19, 2013 11:14 pm

My hubby recently purchased a Canon Image Class MF4800 Series (4890dw, I think -- my over-50 eyes are having trouble reading the writing :mrgreen: ). Reading the MSDS, I believe it had about 45% ferrite (that's from memory... hopefully it's better than my eyes)

I am in the middle of my first attempt at trying the technique from the book that uses regular paper. It looks promising. I've fired the image on the glass, will soon get a background blank in the kiln, and then combine the two in a third firing.

I'll try to remember to let you know how it goes.

Dana W.

tbach
Posts: 33
Joined: Tue Jan 04, 2011 11:35 pm
Location: Hillsboro, Oregon

Re: HP Cartridges that work for image transfer

Postby tbach » Tue Aug 20, 2013 10:28 am

78A and 5A both work well

Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: HP Cartridges that work for image transfer

Postby Morganica » Tue Aug 20, 2013 1:05 pm

As Dana says, the easiest way to figure this out is to simply read the MSDS. For HP, visit here and look up the one you're interested in: http://www.hp.com/hpinfo/globalcitizenship/environment/productdata/ljmsdsuseng.html?jumpid=reg_R1002_USEN#.UhOallNhvuS
For Canon: http://www.usa.canon.com/cusa/about_canon?pageKeyCode=50, select "product" in the first dropdown and type "toner" in the search box.
For Epson: http://www.epson.com/cgi-bin/Store/support/Supportmsdsmain.jsp
For Xerox: [url]http://www.xerox.com/msds‎[/url] (You need to know the product family to search for , which is lame)
For Brother: http://www.brothertoners.com/brother_MSDS.htm (note that this isn't the official Brother site, it's a toner reseller so it may not be up to date)

Section 3 (Composition) of the MSDS will list percentage of materials in a particular toner. You're looking for "ferrite." Some manufacturers will list it as iron oxide, ferrous oxide or FeO. (Basically, if it says iron or ferr-something, that's the percentage you want) If you see words in the list like "polymer," without any reference to iron, it's the wrong toner.

The more FeO in the toner, the better it works for image transfer. Once you have the MSDS--and they're required to be published for any product sold in the US--all you have to do is make sure it has the minimum percentage you need for your application...for that particular toner.

Do not assume that all toners for a particular printer model, brand and offmarket, contain the same percentage of FeO--check every time the product part number. Sometimes they may not contain any at all, and sometimes a manufacturer can change toner formulations.
Last edited by Morganica on Mon Aug 26, 2013 6:18 pm, edited 1 time in total.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)

Dianne Van de Carr
Posts: 17
Joined: Sun Mar 09, 2003 3:43 pm
Location: Carmichael, CA
Contact:

Re: HP Cartridges that work for image transfer

Postby Dianne Van de Carr » Sun Aug 25, 2013 11:44 pm

I am confused by all of this.
I purchased a HP1212 LaserJet printer and according to MSDS it contains less than 50% Styrene Acrylate Copolymer and less than 45% Ferrite. Will it work or should I return the printer? It appears that the older printers use toner with higher ferrite percentages. What to do, what to do???

Dianne

Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: HP Cartridges that work for image transfer

Postby Morganica » Mon Aug 26, 2013 12:02 am

if it has some percentage of iron, ie ferrite, try it, and see how it works for your application. If it doesn't work, you may need to buy a toner richer in iron for it. More than likely there is one.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)

Dianne Van de Carr
Posts: 17
Joined: Sun Mar 09, 2003 3:43 pm
Location: Carmichael, CA
Contact:

Re: HP Cartridges that work for image transfer

Postby Dianne Van de Carr » Mon Aug 26, 2013 4:27 pm

Thanks! I ordered a MICR cartridge too just in case.
Dianne

Virginia Robinson
Posts: 1
Joined: Tue Sep 03, 2013 10:59 am

Re: HP Cartridges that work for image transfer

Postby Virginia Robinson » Tue Sep 03, 2013 6:30 pm

:?: Does anyone know what kind of rinter and cartridges will work to make a decal that can then b fired onto ceramic and pottery and glass


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 8 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com