Photo transfer results

Postby JestersBaubles » Wed Sep 04, 2013 11:15 pm

I promised I would post a picture of the photo transfer I did with the Canon Imageclass printer. Finally pulled it out of the kiln today, and wrote a quick blog post:

http://jestersbaubles.blogspot.com/2013/09/photo-transfer-on-glass.html

Please excuse the poor quality photograph (it really DOES look better than the pic), but I wanted to get this "out there" before I get too busy/forget.

Dana

If you have no time for blog posts, I've attached the image :mrgreen:

phototransfer-fused4-small.jpg

Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 13 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com