I promised I would post a picture of the photo transfer I did with the Canon Imageclass printer. Finally pulled it out of the kiln today, and wrote a quick blog post:

http://jestersbaubles.blogspot.com/2013 ... glass.html

Please excuse the poor quality photograph (it really DOES look better than the pic), but I wanted to get this "out there" before I get too busy/forget.

Dana

If you have no time for blog posts, I've attached the image :mrgreen: