Postby Geo » Wed Sep 11, 2013 2:47 pm

I'm using MR97 spray on a stainless steel bowl for draping. The instructions say to brush the mold and spray on a single coat for subsequent firings. After my first fire, the mold still looks very well coated and I'm wondering how necessary it is to repeat the MR97 coat before firing again.

JestersBaubles
Posts: 692
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: MR97

Postby JestersBaubles » Wed Sep 11, 2013 3:36 pm

I never brush the mold. Just lightly recoat.

Dana

Geo
Posts: 48
Joined: Mon Jul 07, 2003 8:54 am

Re: MR97

Postby Geo » Thu Sep 12, 2013 9:05 am

Thank you!


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 45 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com