24" inch round Kiln Shelves - WarmGlass.com

24" inch round Kiln Shelves

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Tony Smith, Brad Walker

Post Reply
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

24" inch round Kiln Shelves

Postby twin vision glass » Mon Oct 28, 2013 2:36 pm

Hello to everyone. I am looking for 24 inch round kiln shelves for my deep skutt kiln. I really would like it in one piece and not joining as it is important to have a completely full shelf. I will waite patiently till someone might have some suggestions.
Les
Upon further reflection, perhaps large square could be cut. BUT any large kiln shelf that would fit in a 26" wide Skutt.

Victoria Balva
Posts: 17
Joined: Thu Sep 03, 2009 10:18 am

Re: 24" inch round Kiln Shelves

Postby Victoria Balva » Mon Oct 28, 2013 6:10 pm

Glass ceilings www.crowndome.com
Contemporary glass www.artisticlinestudio.com

twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: 24" inch round Kiln Shelves

Postby twin vision glass » Mon Oct 28, 2013 9:25 pm

Victoria , thank you thank you. I have ordered a 26 inch which gives me lots of options. I truly appreciate the help. Leslie

twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: 24" inch round Kiln Shelves

Postby twin vision glass » Mon Oct 28, 2013 10:11 pm

Well I have now ordered also a few amazing drop out molds from Laurie Spray to go with my new shelf. YEAH!!!!!!!!!!! went to the hot shop and pulled some cane so will have alot of fun designing for these molds and new shelves.
Leslie :-k :D

S.TImmerman
Posts: 235
Joined: Wed Nov 25, 2009 9:23 am
Location: San Diego ,Ca

Re: 24" inch round Kiln Shelves

Postby S.TImmerman » Tue Oct 29, 2013 4:10 am

Yes! Thank you! I needed a new shelf too. My golden retriever went running though my studio and my shelves were standing on end as I just primed them. Bang! Two fell over and one broke.

I'm curious what they use those 1 3/4" dia. Solid Silicon Carbide Posts for? Kiln posts?

Thanks!

twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: 24" inch round Kiln Shelves

Postby twin vision glass » Tue Oct 29, 2013 11:02 am

I LOVE the Euclid company as I do believe they are Canadian AND that is the kiln type I use at Uroboros Glass Company when I go down for residency's . It is a large and wonderful top and bottom element kiln . So incredible to do large work in. (and they are so very very kind and helpful) . It is a dream place to go. Nothing but wonderful things to say about Uroboros. :) Les

Terry Gallentine
Posts: 162
Joined: Mon Jul 19, 2004 2:08 pm
Location: River Falls, WI
Contact:

Re: 24" inch round Kiln Shelves

Postby Terry Gallentine » Tue Nov 05, 2013 10:28 pm

I use Corelite shelves in my Euclid clamshells. The shelves are 25.5 inches in diameter and fit nicely in the 29" diameter kilns.

twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: 24" inch round Kiln Shelves

Postby twin vision glass » Wed Nov 06, 2013 3:35 pm

I have always wanted to try those shelves. Do you like them with Kiln Wash as the way I work I cannot use fiber. Les

Terry Gallentine
Posts: 162
Joined: Mon Jul 19, 2004 2:08 pm
Location: River Falls, WI
Contact:

Re: 24" inch round Kiln Shelves

Postby Terry Gallentine » Wed Nov 06, 2013 8:43 pm

I never use fiber. I quick heat the shelf in the kiln to 500 degrees, take it out and spray a thin mix of kiln wash on it while it is hot. I have fired these shelves at least a hundred times and have had no problems with them. I elevate the shelf a couple of inches from the kiln floor with small softbrick posts.

twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: 24" inch round Kiln Shelves

Postby twin vision glass » Sat Nov 09, 2013 4:49 pm

I am a HUGE fan of your work and find you to be an inspiration for everyone here I am sure. Thank you for your input as it is greatly appreciated. Les

dee
Posts: 302
Joined: Tue Mar 11, 2003 5:20 pm
Location: Atlanta GA
Contact:

Re: 24" inch round Kiln Shelves

Postby dee » Thu Nov 14, 2013 11:11 pm

i have corelite shelves for both mama - 24" jen ken "round" - and papa - 28" square olympic - kilns. LOVE them! i only use kiln wash on them, often cheat and just add 4 layers new kiln wash on existing kiln wash unless i've had opal glass pull up the kilnwash. they clean well with a paint scraper - i sometimes follow up with a coarse sanding sponge.
D
Dee Janssen
Unicorn's Creations Studio
http://ucjewelry.com
dee@ucjewelry.com


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 53 guests

Warm Glass