Sandblaster or WBS?

Postby smallbitz » Wed Jan 01, 2014 10:54 am

Happy New Year to all!

I am adding to my home (garage) studio, and trying to decide on a wbs or a sandblaster...Not sure which one I would get the most use out of. Most of the work I do is functional (bowls, platters, wall hangings, etc), usually nothing over 20" or so. I do not do casting. I do a very small amount of jewelry. Any suggestions?

JestersBaubles
Posts: 698
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Sandblaster or WBS?

Postby JestersBaubles » Wed Jan 01, 2014 11:59 am

I guess it depends upon what type of coldworking you want to do :mrgreen: . They are two very different tools.

If you are creating functional pieces, that probably means you need to clean up edges and flatten bottoms. If that's the case, I would get the wet belt sander (or a flat lap).

2 cents,

Dana W.

Marty
Posts: 854
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Sandblaster or WBS?

Postby Marty » Wed Jan 01, 2014 10:02 pm

Those are both serious commitments of time and money and space. Aren't there studios nearby where you can rent time on both? I took my stuff to a rented sandblaster about an hour away until the inconvenience answered the question.

charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: Sandblaster or WBS?

Postby charlie » Wed Jan 01, 2014 11:31 pm

buy the tool that addresses the problems you are having, or what you want to do to the glass.

these 2 tools don't have any overlapping capabilities, whereas a wbs and flat lap have some, making that decision a harder one. we can't answer your question because we don't know what problems you are having, nor whether you can borrow/rent/trade time on one or the other more easily in your location.

Jeanne
Posts: 75
Joined: Wed Aug 20, 2003 8:16 am
Location: NJ

Re: Sandblaster or WBS?

Postby Jeanne » Thu Jan 02, 2014 12:28 pm

As Charlie said, these tools do different things. I was able to get a new inexpensive blast cabinet (about 24" wide) that works for the size pieces I do. Cost about $200. The Compressor was more money (around $350). I was able to get a Somaca wet belt sander off of Craigslist (not that easy to find used btw) for under $300. Considering what they cost new, I was thrilled beyond words.

Bert Weiss
Posts: 2338
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Sandblaster or WBS?

Postby Bert Weiss » Thu Jan 02, 2014 1:28 pm

The good news is that small scale work uses small scale tools. You may well get away with a diamond wet grinder with a 4" flat lap for grinding, and a little sandblaster designed for cleaning small parts.

I'm sure some of the glass jewelry makers here can chime in with what tools work well for them.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

smallbitz
Posts: 154
Joined: Sat Jun 27, 2009 8:44 am
Location: Florida

Re: Sandblaster or WBS?

Postby smallbitz » Thu Jan 02, 2014 9:52 pm

Thanks so much for the suggestions. I really don't have any studios near me to rent time on either of these tools. I suppose that I really do more edge work on sinks, thick bowls, strip work and drop outs so I guess that a wbs would be a more useful purchase for me. Most of what I would use a sandblaster for I could probably do by hand...

lorimendenhall
Posts: 91
Joined: Wed Apr 10, 2013 8:54 pm
Location: Orange County, CA
Contact:

Re: Sandblaster or WBS?

Postby lorimendenhall » Fri Jan 03, 2014 7:00 pm

but a sandblaster is so fun!!!! I actually want both of these things too...


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 46 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com