Bridge saws - WarmGlass.com

Bridge saws

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Tony Smith, Brad Walker

Post Reply
Marty
Posts: 853
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Bridge saws

Postby Marty » Wed Jan 29, 2014 1:09 pm

Anyone have any experience with 10" to 14" bridge (or rail) tile saws? The manual ones with 3' to 4' spans, not the gigantic ones used for stone.

charlie holden
Posts: 260
Joined: Thu Mar 13, 2003 8:26 pm
Location: Atlanta

Re: Bridge saws

Postby charlie holden » Wed Jan 29, 2014 2:34 pm

I have an MK 212 with a 36 inch span and a 10 inch blade. It's great for long cuts on thin pieces, not so great for cutting odd angles and depths -- like cutting the neck off a curvy blown piece.

My only complaint is that when I bought it they advertised that it had a 3 inch deep cut, which is not true. There is 3 inches at the blade but less clearance than that under the motor -- more like 2 1/4 inches. And the amount you can raise the saw off the bed is very limited compared to some of the chop saw styles.

Marty
Posts: 853
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Bridge saws

Postby Marty » Wed Jan 29, 2014 5:51 pm

Thanks, Charlie. How much can you raise the blade off the bed?

Rick Wilton
Posts: 273
Joined: Sat Oct 25, 2003 8:18 pm
Location: Calgary, Canada
Contact:

Re: Bridge saws

Postby Rick Wilton » Wed Jan 29, 2014 8:02 pm

They have two different ones on display at home depot here. You may be have similar there, you can inspect them much better than a pic online.

I've seen them for rent at the local tool rental place also, might be worth a rent. If you rent be careful about their blades as they'll hose you for any useage of the blade. I rented once and they tried to charge me than the price as a new blade and I only a few pieces.
Rick Wilton

dee
Posts: 302
Joined: Tue Mar 11, 2003 5:20 pm
Location: Atlanta GA
Contact:

Re: Bridge saws

Postby dee » Sun Feb 02, 2014 1:39 pm

Also check places that sell tile flooring, we have a place here, floor and decor, that has different brands of tile saws than what home depot has and i've been looking at one over there off and on...
D
Dee Janssen
Unicorn's Creations Studio
http://ucjewelry.com
dee@ucjewelry.com

Cheryl
Posts: 239
Joined: Sun Mar 09, 2003 7:56 pm
Location: Tallahassee FL
Contact:

Re: Bridge saws

Postby Cheryl » Fri Feb 21, 2014 8:52 pm

i use an IMER. love some things about it, not thrilled about others - like blade depth.
"Every artist was first an amateur."

--Ralph Waldo Emerson


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 30 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com