What is the difference in the back of the glass fired on hotline hi fire vs Bullseye vs Papyros?

I have been using papyros( switched from TF becuase easier to clean up) in my small kiln and Primo Primer (it gives a very smooth back) on my molds. I want to omit the papyros if I can get a smooth back.

I just got JenKen oval13 just arrived with some of their" sir ramic" kiln wash that is course feeling - don't care for it. How does the BE compare to the Hotline HiFire?

Thanks,
Chris

tgotch
Posts: 36
Joined: Mon Nov 14, 2011 11:04 pm

Re: BE vs Hotline Hifire ?

Postby tgotch » Fri Feb 14, 2014 3:34 pm

Here is a good comparison of primers:

https://docs.google.com/viewer?a=v&q=ca ... RFPnB2xjWQ

chrisk
Posts: 13
Joined: Tue Nov 04, 2008 12:45 am

Re: BE vs Hotline Hifire ?

Postby chrisk » Fri Feb 14, 2014 8:49 pm

Thank you - I appreciate all the detailed comparisions.
Chris


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 41 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron