Posted: Fri Feb 14, 2014 2:28 am
What is the difference in the back of the glass fired on hotline hi fire vs Bullseye vs Papyros?
I have been using papyros( switched from TF becuase easier to clean up) in my small kiln and Primo Primer (it gives a very smooth back) on my molds. I want to omit the papyros if I can get a smooth back.
I just got JenKen oval13 just arrived with some of their" sir ramic" kiln wash that is course feeling - don't care for it. How does the BE compare to the Hotline HiFire?
Thanks,
Chris