Postby chrisk » Mon Mar 03, 2014 6:03 pm

I need some schedule help/advice, please. All my kilns are JenKen - the old kiln is a 16" fiber Bonnie Glo with side elements, my new oval 24x39 has side & top elements. I am attaching a pic of my first fire - all bulleye 2 layers. The 10.5 square was perfect as was the 6" retro square. The aqua coasters were only a little curved on the sides (I had to cold work a bit) and the red & black were extremely distorted and the black glass was overcooked - the color is strange sort of brownish.
The schedule I used is:
Ramp Degrees Hold/min
1) 300 - 500 - 02
2) 500 - 1150 - 05
3) 325 - 1225 - 50 bubble squeeze
4) 400 - 1480 - 10 ( my top temp is 1490 in the Bonnie Glo)
5) Full - 900 - 60
6) 100 - 700 - 2

2nd question - going to the large kiln with top elements are temps usually lower for all (fire polish, tac fuse/slump) compared to the smaller kilns with only side elements.

Thank you,
Chris
first fire.jpg
first fire.jpg (41.05 KiB) Viewed 1945 times

Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 19 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com