Firepolish after slump?
Moderators: Brad Walker, Tony Smith
Firepolish after slump?
I want to make some small coldworking changes to a piece that I have already slumped. I know it's not the best idea to slump and firepolish in the same firing, but what about firepolishing after I've already slumped? Okay to do it if I put it back in the mold?
-
Brad Walker
- Site Admin
- Posts: 1540
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Firepolish after slump?
What's the shape of the mold?
Re: Firepolish after slump?
It's a rather organic, wavy piece. About 2 1/2" deep rectangle - no lip, like a flag that will be put on edge to be displayed horizontally on a table on a stand. 6mm thick.
Re: Firepolish after slump?
It's fine to firepolish and slump in the same schedule if the work supports it. Since you'll be going hotter and probably longer than a standard slump, that's the real question.
If the glass can continue sliding down the mold so that it begins to puddle on the bottom, then it's a bad idea because your the glass will deform. If the mold is relatively flat, or in some way stops additional slumping from happening, then it's OK. I do that kind of slump/firepolish a lot.
If the glass can continue sliding down the mold so that it begins to puddle on the bottom, then it's a bad idea because your the glass will deform. If the mold is relatively flat, or in some way stops additional slumping from happening, then it's OK. I do that kind of slump/firepolish a lot.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Re: Firepolish after slump?
Thanks. I don't think reshaping will be a problem in this mold. I'm going to give it a try and just keep my eye on it!
Re: Firepolish after slump?
The firepolish/slump worked great. I did watch it carefully. I can see how it would NOT work in a steep bowl mold or some other shapes. It really does depend on the mold. Tried to upload a photo, but I can't seem to get it to upload. Never used to have trouble with that...