Postby smallbitz » Thu Mar 13, 2014 7:05 am

I want to make some small coldworking changes to a piece that I have already slumped. I know it's not the best idea to slump and firepolish in the same firing, but what about firepolishing after I've already slumped? Okay to do it if I put it back in the mold?

Brad Walker
Site Admin
Posts: 1374
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Firepolish after slump?

Postby Brad Walker » Thu Mar 13, 2014 9:06 am

What's the shape of the mold?

smallbitz
Posts: 154
Joined: Sat Jun 27, 2009 8:44 am
Location: Florida

Re: Firepolish after slump?

Postby smallbitz » Thu Mar 13, 2014 9:22 am

It's a rather organic, wavy piece. About 2 1/2" deep rectangle - no lip, like a flag that will be put on edge to be displayed horizontally on a table on a stand. 6mm thick.

Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Firepolish after slump?

Postby Morganica » Thu Mar 13, 2014 6:22 pm

It's fine to firepolish and slump in the same schedule if the work supports it. Since you'll be going hotter and probably longer than a standard slump, that's the real question.

If the glass can continue sliding down the mold so that it begins to puddle on the bottom, then it's a bad idea because your the glass will deform. If the mold is relatively flat, or in some way stops additional slumping from happening, then it's OK. I do that kind of slump/firepolish a lot.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)

smallbitz
Posts: 154
Joined: Sat Jun 27, 2009 8:44 am
Location: Florida

Re: Firepolish after slump?

Postby smallbitz » Fri Mar 14, 2014 6:27 am

Thanks. I don't think reshaping will be a problem in this mold. I'm going to give it a try and just keep my eye on it!

Jeanice
Posts: 35
Joined: Sun Jan 01, 2012 1:24 pm
Location: Wyoming, USA

Re: Firepolish after slump?

Postby Jeanice » Sat Mar 15, 2014 11:56 am

Let us know how it goes. And maybe a photo?
Jeanice

smallbitz
Posts: 154
Joined: Sat Jun 27, 2009 8:44 am
Location: Florida

Re: Firepolish after slump?

Postby smallbitz » Mon Mar 17, 2014 9:41 am

The firepolish/slump worked great. I did watch it carefully. I can see how it would NOT work in a steep bowl mold or some other shapes. It really does depend on the mold. Tried to upload a photo, but I can't seem to get it to upload. Never used to have trouble with that...


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 52 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron