photo decals - black and white
Posted: Thu Mar 20, 2014 10:03 pm
by Terry Ow-Wing
Hand any one used photo decals from Fusion?
http://www.fusionheadquarters.com/product_p/decpap.htm
It says"If your printer is a Black and White HP or Canon Laser Printer or copier and has absolutely NO capability of printing in color… it will work."
Thanks -
Re: photo decals - black and white
Posted: Thu Mar 20, 2014 10:26 pm
by Barry Kaiser
Best I can tell, this is the standard decal paper available in many places including our web store (see below).
Many canon printers do have the iron oxide in the toner, but some do not. You are pretty safe with HP black only printer
Note: you still get the "sepia" color, also known as rust.
Barry
Re: photo decals - black and white
Posted: Fri Mar 21, 2014 10:27 pm
by Terry Ow-Wing
Barry Kaiser wrote:Best I can tell, this is the standard decal paper available in many places including our web store (see below).
Many canon printers do have the iron oxide in the toner, but some do not. You are pretty safe with HP black only printer
Note: you still get the "sepia" color, also known as rust.
Barry
thanks for the answer I just remember a ton of talk about which printers had the iron oxide and if there was enough .