Postby Miriam Silburt » Mon Mar 24, 2014 10:00 am

Can you fire silver with glass?

Barry Kaiser
Posts: 286
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: silver and glass

Postby Barry Kaiser » Mon Mar 24, 2014 10:15 am

Yes, but it does depend on the thickness of the silver and the glass it is fused with (reactivity)
I screen print silver slip all the time on to BE1401.
Difficult to cap.....yellows.

pendant1043.jpg
pendant1044.jpg

lorimendenhall
Posts: 91
Joined: Wed Apr 10, 2013 8:54 pm
Location: Orange County, CA
Contact:

Re: silver and glass

Postby lorimendenhall » Mon Mar 24, 2014 6:04 pm

if you use fine silver it will stay bright silver colored. if you use sterling silver it turns ugly. I embed fine silver hangers into pendants all the time.

JestersBaubles
Posts: 696
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: silver and glass

Postby JestersBaubles » Tue Mar 25, 2014 4:58 pm

Make sure to take into considerations the reactions due to the silver. You might want to look at a blog post I did on Bullseye reactive glass:

http://jestersbaubles.blogspot.com/2014/01/bullseye-reactive-glass.html

Dana W.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 29 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com