Dichrochic
Posts: 2
Joined: Mon Feb 19, 2007 12:06 am
Location: California

Fire Polishing small jewelry pieces

Postby Dichrochic » Mon Apr 28, 2014 1:59 am

Hello, I used a mold to to do a couple of jewelry items and some of the edges came out a little bit rough. I have been told I could just use my grinder, would I use my grinder or would it be better to use my Gryphon Wet Belt Sander? if so, on what number belt should I use? also, would I need to fire polish after ?
Any, help would be much appreciated, thank you.

Drewcilla
Posts: 60
Joined: Fri Apr 11, 2008 9:10 am

Re: Fire Polishing small jewelry pieces

Postby Drewcilla » Mon Apr 28, 2014 12:09 pm

I usually just use my grinder for small things like jewelry and fire polish afterwards. If they need a lot of work, e.g., changing the basic shape, it's good to start with a coarse grit and finish up with a finer grit head (220 or 600). In any case, drop the piece into water after grinding to keep grinder scum from getting embedded on the edges or scrub them right away. Otherwise, you can get an ugly edge where you ground them after you fire polish.

Barry Kaiser
Posts: 285
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: Fire Polishing small jewelry pieces

Postby Barry Kaiser » Mon Apr 28, 2014 1:23 pm

also suggest you use a borax based devit agent when doing the fire polish.

Barry

Dichrochic
Posts: 2
Joined: Mon Feb 19, 2007 12:06 am
Location: California

Re: Fire Polishing small jewelry pieces

Postby Dichrochic » Mon Apr 28, 2014 5:04 pm

Hello, again thank you so much for the help. smooches


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 51 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron