All of a sudden my kiln wash is sticking to my pieces of fused glass. Not sure why. I've been using the same kiln boards and kiln wash for years, and it never used to stick. Now it's sticking. Not sure why. Could it be because the boards are getting older? I'm using the same kiln wash (from Bullseye) and applying it the same way.

Any thoughts?

Drew

Marty
Posts: 853
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: kiln wash sticking

Postby Marty » Mon Jul 28, 2014 12:49 pm

My first thought is that your thermocouple is acting up- have you noticed any changes in the fired glass that would be due to excess heat?
Second thought- new batch of kw?

AJK25
Posts: 39
Joined: Wed Jul 20, 2005 12:49 pm

Re: kiln wash sticking

Postby AJK25 » Mon Jul 28, 2014 12:58 pm

i think the thermocouple is ok. Might be the kiln wash.

Thanks Marty.

Mark Kemp
Posts: 59
Joined: Mon Mar 10, 2003 11:57 am
Location: Corvallis, Oregon
Contact:

Re: kiln wash sticking

Postby Mark Kemp » Tue Jul 29, 2014 9:43 pm

I got a new tub of BE kilnwash at some point, and it looked different -- color was still pinkish, but different than before. Enough so, I checked with them to make sure it was the real stuff. But after I started using it, I had some sticking problems, even on cathedrals. I had never needed to prefire shelves before that, but I started preheating them to about 300F to drive off water, and haven't had much problem since then.
Find peace in your heart.

www.azurefire.etsy.com

AJK25
Posts: 39
Joined: Wed Jul 20, 2005 12:49 pm

Re: kiln wash sticking

Postby AJK25 » Wed Jul 30, 2014 10:35 am

thanks


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 44 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com