So, I am in the process of making a fused glass font bowl for my church. They want the opening to be 12" with a lip and 6" deep. I have purchased a drop ring from Laurie Spray along with a 18 1/2" steel ring. I figured 3" overhang would be enough to hold. Laurie's rings have a lip on one side to help have the glass remain on the ring and NOT fall through. I also was nervous so I ordered a 20"metal ring from slumps, just in case I don't have a big enough lip to go by.
Anyway, attempt #1, I went too fast (200º/hr on 1st ramp to 1200. I also used the kiln that does not allow top elements to be turned off. Major fail.
Attempt #2, new, larger kiln (Olympic) that allows me to keep top elements off, Scheduled ramp at 150º/hr to 1200 and hold for as long as it takes. Kept peeking every 5 minutes, after 1 hour, glass had fallen through. This practice piece was 15" with only a 1 1/2" gap around to hold the rim. The glass lasted for 45 minutes before it sunk to the floor. (they want it 6-7"deep. I may settle for 4-5")
Attempt #3: Olympic kiln with top elements turned off and piece center in kiln, raised 7" from shelf. This piece of glass is 20" and 9mm thick. My schedule:
50 - 1100 - 45
50 - 1200 - As long as needed (was going to program 2 hours and delete the after peeking every 5 minutes.
once reached AFAP - 900 - 2:00
150 - 750 - off

The 20" circle should give me enough lip to hold the piece in place, right? Any suggested are greatly appreciated.

Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 14 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron