Postby sheila » Tue Sep 16, 2014 10:52 pm

Need to know ASAP:

Will BE 1332-50 strike if capped with tekta 3.0- rainbow irid?? or do I need to have the clear on the bottom? I'll full fire to 1480, per your suggested program, with 45 min. hold at 1225.

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Capping a fuchsia striker 1332-50

Postby Valerie Adams » Wed Sep 17, 2014 12:17 am

Yes, it'll strike but the rainbow irid with obscure the color a bit. Although Tekta isn't available with an irid coating as far as I know, so you must be using 1101-0031.

sheila
Posts: 11
Joined: Wed Apr 02, 2003 2:03 pm
Location: Seward, Alaska

Re: Capping a fuchsia striker 1332-50

Postby sheila » Wed Sep 17, 2014 12:36 am

Correct..1101-31. Prefer to use clear on top to make tight lines in pieces below. So, fuchsia will fully strike if capped. Thanks!


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 44 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com