Capping a fuchsia striker 1332-50
Posted: Tue Sep 16, 2014 10:52 pm
Need to know ASAP:
Will BE 1332-50 strike if capped with tekta 3.0- rainbow irid?? or do I need to have the clear on the bottom? I'll full fire to 1480, per your suggested program, with 45 min. hold at 1225.
Will BE 1332-50 strike if capped with tekta 3.0- rainbow irid?? or do I need to have the clear on the bottom? I'll full fire to 1480, per your suggested program, with 45 min. hold at 1225.