Scratch on final product

Postby Deb » Sun Oct 05, 2014 11:04 pm

After coming home from a show, I noticed a small scratch on top of my item. Normally, I would put it back in the kiln and polish it but I have glued cabochons on the bottom with E6000. Any suggestion on how to fix the scratch or how to loosen up E6000 between 2 pieces of glass? Thanks.
Deb

Georgia Novak
Posts: 28
Joined: Wed Jun 04, 2003 2:54 am

Re: Scratch on final product

Postby Georgia Novak » Mon Oct 06, 2014 3:07 pm

soak it in Acetone until loose. Pour the Acetone in a container that you can put a lid on or it will evaporate before it separates the pieces.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 76 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com